FCFC Formosa TAIRIPRO® K3029 PP Impact Copolymer

fcfc tairipro® pp copolymer 25kg package

TAIRIPRO® K3029 PP Impact Copolymer Injection Molding

TAIRIPRO K3029 is an impact copolymer PP resin engineered for high-performance manufacturing. Combining high fluidity (Melt Flow Index: 32 g/10min) and exceptional impact strength (147 kJ/m² at 73°F), it simplifies production of durable, complex parts while reducing cycle times. Ideal for automotive, packaging, and thin-wall applications, this material balances efficiency with reliability.

Associated Documents

ISO Data Sheet
ASTM Data Sheet
UL Product iQ
Processing Data

Typical property data

Physical Properties

Specific Gravity: 0.9 (ISO 1183, 23℃/23℃)

Mechanical Properties
  • Tensile Strength: 21 MPa (ISO 527, 23℃, 50mm/min)
  • Tensile Elongation at Break: >100% (ISO 527, 23℃, 50mm/min)
  • Flexural Modulus: 980 MPa (ISO 178, 23℃)
  • Rockwell Hardness: R-75 (ISO 2039-2, 23℃)
Impact Properties

IZOD Impact Strength (Notched):

  • 69 kJ/m² (ISO 180, 0℉, 4mm)
  • 147 kJ/m² (ISO 180, 73℉, 1/8″)
Thermal Properties

Heat Deflection Temperature: 108℃ (ISO 75/A, Unannealed, 0.455 MPa, 1/4″ thickness)

Flame Characteristics

Combustibility: HB Rating (UL-94, 1.5–3 mm thickness)

Injection Molding
  • Melt Flow Index: 32 g/10 min (ISO 1133, 230℃ × 2.16kg)
  • Molding Shrinkage: 1.4–1.8% (FCFC Method, 23℃)

Features & Benefits

Superior Flow

TAIRIPRO K3029’s high fluidity ensures seamless filling of thin-walled or intricate molds. This reduces warping and shortens cycle times, cutting costs for items like disposable containers or lightweight automotive panels.

Toughness for Demanding Environments

With an IZOD impact strength of 147 kJ/m², K3029 withstands harsh conditions. Perfect for bumpers or industrial components, it resists cracks and impacts, extending product lifespan.

Heat Resistance & Stability

A heat deflection temperature of 108°C ensures stability in high-heat scenarios. Use it for under-hood automotive parts or reusable food containers without compromising structural integrity.

fcfc tairipro® pp copolymer 25kg package

Use & applications

  • Automotive Bumpers: High impact strength absorbs collisions, reducing repair costs.
  • Thin-Wall Packaging: High fluidity enables detailed, lightweight designs (e.g., food containers).
  • Engine Components: Heat resistance ensures reliability in under-hood parts.
tairipro k3029 pp resin application

Send Us a Message