FCFC Formosa TAIRIPRO® K4515 PP Random Copolymer

fcfc tairipro pp resin random copolymer

TAIRIPRO® K4515 Random Copolymer PP Injection Molding

With high clarity, anti-static properties, and excellent chemical resistance, this TAIRIPRO® K4515 PP Resin material is ideal for injection-molded applications requiring durability and aesthetic appeal. Its balanced mechanical strength and ease of processing make it a trusted choice for industrial and consumer goods.

Associated Documents

ISO Data Sheet
ASTM Data Sheet
UL Product iQ
Processing Data

Typical property data

Physical Properties

Specific Gravity: 0.9 (ISO 1183, 23°C/23°C)

Mechanical Properties
  • Tensile Strength: 30 MPa (ISO 527, 23°C, 50 mm/min)
  • Tensile Elongation at Break: >200% (ISO 527, 23°C, 50 mm/min)
  • Flexural Modulus: 1127 MPa (ISO 178, 23°C)
  • Rockwell Hardness: R-95 (ISO 2039-2, 23°C)
Impact Properties
  • IZOD Impact Strength: 59 kJ/m² (ISO 180, 23°C, Notched, 1/8″)
  • IZOD Impact Strength: 59 kJ/m² (ISO 180, 23°C, Notched, 4mm)
Thermal Properties

Heat Deflection Temperature: 95°C (ISO 75/A, unannealed, 0.455 MPa, 1/4″ thick, 120°C/hour)

Optical Properties

Features: High Clarity

Flame Characteristics

Combustibility: HB, 1.5 ~ 1.65 mm (UL-94, File No. E162823)

Injection Molding

Melt Flow Index (MFI): 18 g/10 min (ISO 1133, 230°C × 2.16 kg)

Features & Benefits

High Crystal-Clear Durability

TAIRIPRO K4515 delivers high transparency comparable to glass, perfect for products where visual inspection matters (e.g., medical containers). Its clarity remains intact even after repeated sterilization, reducing defects in critical applications.

Static-Free Performance

Built-in anti-static properties minimize dust attraction during production and end-use. This feature is crucial for electronics packaging or cleanroom environments, ensuring contamination-free surfaces and smoother workflows.

Chemical Resistance

Withstand exposure to oils, detergents, and mild acids without degradation. This makes K4515 PP resin ideal for automotive components or household cleaning tools that face frequent chemical contact.

fcfc tairipro pp resin random copolymer

Use & applications

High-Transparency Containers

Used in medical IV bottles and labware where clarity ensures safe liquid-level monitoring.

Transparent Housewares

Dishwasher-safe food storage boxes that resist staining from oils or sauces.

USP Class VI Approved Components

Medical trays and surgical instrument housings requiring biocompatibility and sterilizability.