Tairipro K8025 is a high-performance impact copolymer PP resin engineered. Combining high impact strength (up to 123 kJ/m²) and high fluidity (Melt Flow Index: 28 g/10 min), it excels in demanding applications like automotive parts, appliance components, and industrial tools. Ideal for complex molds and high-stress environments.

Associated Documents

ISO Data Sheet
ASTM Data Sheet
UL Product iQ
Processing Data

Typical property data

Physical Properties
  • Melt Flow Index: 28 g/10 min (ISO 1133, 230℃ × 2.16 kg)
  • Specific Gravity: 0.9 (ISO 1183, 23℃/23℃)
Mechanical Properties
  • Tensile Strength: 22 MPa (ISO 527, 23℃, 50 mm/min)
  • Tensile Elongation at Break: >200% (ISO 527, 23℃, 50 mm/min)
  • Flexural Modulus: 1078 MPa (ISO 178, 23℃)
  • Rockwell Hardness: R-80 (ISO 2039-2, 23℃)
Impact Properties
  • IZOD Impact Strength (Notched):
  • 61 kJ/m² (ISO 180, 0℉, 4 mm)
  • 123 kJ/m² (ISO 180, 73℉, 1/8″)
Thermal Properties
  • Heat Deflection Temperature: 110℃ (ISO 75/A, Unannealed, 0.455 MPa, 1/4″ thick, 120℃/h)
Flame Characteristics
  • Combustibility: HB (UL-94, File No. E162823, 1.5 mm)
Injection Molding
  • Molding Shrinkage: 1.4–1.8% (FCFC Method, 23℃)

Features & Benefits

Unmatched Impact Resistance

Tairipro K8025 delivers IZOD impact strength of 123 kJ/m² at room temperature, making it perfect for parts exposed to shocks or drops. Think automotive bumpers or washing machine agitators—materials stay intact even under harsh conditions.

Effortless Moldability

With a Melt Flow Index of 28 g/10 min, this tarflon PP Resin flows smoothly into intricate molds. Reduce cycle times and minimize defects in thin-walled components like tool box latches or appliance housings.

Heat & Weight Efficiency

A heat deflection temperature of 110°C ensures stability in high-heat environments, such as dishwasher parts. Plus, its specific gravity of 0.9 keeps products lightweight without sacrificing strength—critical for automotive weight reduction.

tairipro k8025 pp resin

Use & Applications

  • Automotive Parts: Bumpers, dashboards, and interior panels requiring crash resistance and lightweight design.
  • Washing Machine Parts: Agitators, lids, and detergent trays that endure vibration and hot water cycles.
  • Tool Boxes: Durable latches, hinges, and casings resistant to drops and outdoor conditions.
tairipro pp resin k8025 application

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.