FCFC Formosa TAIRIPRO® T4002 PP Random Copolymer

fcfc tairipro pp resin random copolymer

TAIRIPRO® T4002 Random Copolymer PP Film Grade

TAIRIPRO T4002 is a high-performance PP random copolymer resin designed for extrusion and blow molding. Combining good transparency and excellent chemical resistance, it offers durability and versatility. T4002 ensures consistent quality across packaging, automotive, and consumer goods sectors.

Associated Documents

ISO Data Sheet
ASTM Data Sheet
Processing Data

Typical property data

Physical Properties
  • Melt Flow Index: 1.6 g/10 min (ISO 1133, 230℃ × 2.16 kg)
  • Specific Gravity: 0.9 (ISO 1183, 23℃/23℃)
Mechanical Properties
  • Tensile Strength: 25 MPa (ISO 527, 23℃, 50 mm/min)
  • Tensile Elongation at Break: >200% (ISO 527, 23℃, 50 mm/min)
  • Flexural Modulus: 833 MPa (ISO 178, 23℃)
  • Rockwell Hardness: R-85 (R-scale, ISO 2039-2, 23℃)
Impact Properties
  • IZOD Impact Strength: 78 kJ/m² (ISO 180, 23℃, Notched, 1/8″ and 4 mm)
Thermal Properties
  • Heat Deflection Temperature: 85℃ (ISO 75/A, Unannealed, 0.455 MPa, 1/4″ thick, 120℃/h)
Optical Properties
  • Good transparency (Qualitative feature)
Injection Molding
  • Molding Shrinkage: 1.5–2% (FCFC Method, 23℃)

Features & Benefits

Crystal-Clear Durability

With 85°C heat deflection temperature and >200% elongation, T4002 maintains structural integrity under stress, making it perfect for transparent containers exposed to heat or impact.

Chemical & Moisture Resistance

It resists acids, alkalis, and solvents, ensuring long-lasting performance in harsh environments like chemical storage tanks or automotive fluid components.

Easy Processing Flexibility

Optimized 1.6 g/10min melt flow rate allows smooth extrusion and blow molding, reducing energy consumption and production downtime.

fcfc tairipro pp resin random copolymer

Use & Applications

Blow Molding

Ideal for producing clear bottles, containers, and other hollow articles requiring transparency and chemical resistance, Automotive fuel tanks and air ducts.

Sheet Extrusion

Suitable for manufacturing transparent sheets used in packaging, signage, and protective barriers.

tairipro t4002 pp resin application

Send Us a Message