Plastic Granules
TAIRIREX® GP550N GPPS Resin General Grade
TAIRIREX GP550N is a high molecular weight GPPS resin designed for exceptional clarity, rigidity, and processability. Ideal for injection molding and extrusion, this TAIRIREX PS resin ensures durable, visually appealing solutions for packaging, medical containers, and industrial sheets like XPS or PSP.
Associated Documents
ISO Data Sheet
ASTM Data Sheet
UL Product iQ
Processing Data
Typical property data
Physical Properties
- Melt Flow Index: 2.6 g/10min (ISO 1133, 200℃ × 5kg)
- Residual Monomer: Max 700 ppm
Mechanical Properties
- Tensile Strength: 48 MPa (ISO 527, 23℃, 20mm/min)
- Tensile Modulus: 3400 MPa (ISO 527, 23℃, 1mm/min)
- Tensile Elongation: 3% (ISO 527, 23℃, 20mm/min)
- Flexural Strength: 84 MPa (ISO 178, 23℃, 2mm/min)
- Flexural Modulus: 3000 MPa (ISO 178, 23℃, 2mm/min)
Impact Properties
- IZOD Impact Strength: 1.6 kJ/m² (ISO 180, 23℃, 4mm, Unnotched)
- Charpy Impact Strength: 9.5 kJ/m² (ISO 179, 23℃, 4mm, Unnotched)
Thermal Properties
- Vicat Softening Point: 103℃ (ISO 306, Annealed 80℃ × 2hr, 4mm, 10N, 50℃/h)
- Heat Deflection Temperature: 98℃ (ISO 75/A, Annealed 80℃ × 2hr, 120℃/h, 1.8 MPa, 4mm)
Flame Characteristics
- Combustibility: UL-94, HB (1.5–1.7 mm thickness)
Features & Benefits
Crystal-Clear Transparency
TAIRIREX GP550N delivers >90% light transmission, perfect for see-through packaging like cosmetic cases or OPS films. Eliminates the need for costly post-processing or coatings.
Reliable Impact Resistance
With a Charpy Impact Strength of 9.5 kJ/m², Formosa GPPS GP550N reduces breakage in fragile items like medicine containers during transport, cutting waste and replacement costs.
Heat-Resistant Performance
A Vicat Softening Point of 103°C ensures stability in warm environments, ideal for XPS insulation boards or disposable cutlery exposed to moderate heat.
Use & Applications
PSP Sheets
Glossy, rigid sheets for disposable food trays or retail signage.
XPS Insulation Boards
Consistent foam structure for energy-efficient building materials.
OPS Shrink Films
High-clarity packaging for electronics or consumer goods.
Medicine Containers
Safe, crack-resistant packaging for pills and syringes.