Formosa TAIRIREX® HP8250 Ningbo

formosa ningbo tairirex® hips 25kg package

TAIRIREX® HP8250 HIPS Resin High Impact Grade

TAIRIREX® HP8250 is a High Impact Polystyrene (HIPS) resin pellet manufactured by Formosa Chemicals Industries (Ningbo) Co., Ltd. , a subsidiary of the Taiwanese plastics giant Formosa Chemicals & Fibre Corporation (FCFC). It is processed via injection molding, and is widely utilized in the manufacturing of electronic appliance housings as well as durable consumer goods.

Associated Documents

ISO Data Sheet
UL Product iQ
Processing Data
FDA (Food Contact Compliance Statement)
EU10 (Food Contact Compliance Declaration)

Typical property data

Physical Properties
  • Melt Flow Index: 5.5 g/10min (ISO 1133, 200°C × 5kg)
Mechanical Properties
  • Tensile Strength: 24 MPa (ISO 527, 23°C, 20mm/min)
  • Tensile Modulus: 2200 MPa (ISO 527, 23°C, 1mm/min)
  • Tensile Elongation: 33% (ISO 527, 23°C, 20mm/min)
  • Flexural Strength: 41 MPa (ISO 178, 23°C, 2mm/min)
  • Flexural Modulus: 2200 MPa (ISO 178, 23°C, 2mm/min)
Impact Properties
  • IZOD Impact Strength: 11 kJ/m² (ISO 180, 23°C, 4mm, Unnotched)
  • Charpy Impact Strength: 8.5 kJ/m² (ISO 179, 23°C, 4mm, Notched)
Thermal Properties
  • Vicat Softening Point: 98°C (ISO 306, Annealed 80°C × 2hr, 10N, 50°C/h)
  • Heat Deflection Temperature: 96°C (ISO 75/A, Annealed 80°C × 2hr, 1.8MPa, 4mm)
Flame Characteristics
  • Combustibility: HB (0.8 ~ 3mm) (UL-94, File No. E162823)
Injection Molding
  • Features: High impact, Normal flow

Use & Applications

  • Electrical Appliance Housings
  • Baby Car Parts
  • LCD Monitor Housings
  • Exercise Equipment
tairirex hips resin hp8250 application

Features & Benefits

High Impact Strength & Durability

TAIRIREX HP8250 HIPS resin offers 11 kJ/m² impact resistance, ideal for products like baby car parts or LCD monitor frames. Its toughness prevents cracks, even under stress, ensuring long-lasting performance.

Easy Moldability for Efficient Production

With a 5.5g/10min melt flow rate, this resin fills molds smoothly, reducing cycle times. Its normal flow suits complex shapes for appliances or exercise gear without compromising detail.

Safe & Heat-Resistant for Daily Use

The material meets UL94 HB flammability standards and handles heat up to 98°C (Vicat). Low residual monomers (700ppm max) make it safe for electronics and child-friendly products.

formosa ningbo tairirex® hips 25kg package

Send Us a Message