HS102R Polycarbonate Granules Medium viscosity General Transparent
Huasheng PC HS102R is a Transparent polycarbonate resin granules. It offers Medium viscosity, good mould release performance, 60 MPa tensile modulus, and 10 g/10min MFR. Ideal for general-purpose, Extrusion, injection molding applications.
Typical property data
Physical Properties
- Melt index (MFR): (300℃/1.2kg) 10±1 g/10min (GB/T 3682.1-2008)
- Density: 1200 kg/m3 (GB/T 1033.1-2008)
- Viscosity average molecular weight (Mv): (Typical value) 20500 g/mol (GB/T 36214.2-2018)
Mechanical Properties
- Tensile strength (yield): ≥60 MPa (GB/T 1040.1-2018)
- Elongation (break): ≥105% (GB/T 1040.1-2018)
- Bending strength: ≥95 MPa (GB/T 9341-2008)
- Izod notched impact strength: ≥65 kJ/m2(GB/T 1043.2-2018)
Optical Performance
- Light transmittance (1mm): 89% ((GB/T 2410-2008)
- b (2mm): 0.1~0.5 (GB/T 39822-2021)
- YI (2mm): 0~1 (GB/T 39822-2021)
Thermal Properties
- Thermal deformation temperature under load (1.8MPa): ≥123 ℃ (GB/T 1634.2-2019)
- Molding shrinkage: 0.6~0.8% (GB/T 39818-2021)
- Vicat softening temperature: ≥140 ℃ (GB/T 1633-2000)
- Glass transition temperature: ≥147 ℃ (GB/T 19466.2-2004)
Flammability Rating
- Limiting oxygen index: 27% (GB/T 2406.1-2008)
- Flame retardant grade: V2 (GB/T 2408-2021)
Use & Applications
- automotive
- electronics
- industrial applications