HS200G Polycarbonate Granules Low Viscosity General

Huasheng HS200G is a low-viscosity polycarbonate resin for injection and extrusion molding. It offers clear transparency, 20 ± 2 g/10 min MFR, 88% transmittance, 60 MPa tensile strength, and V-2 flame rating. Ideal for general-use PC parts.

Associated Documents

TDS - Technical Data Sheet

Typical property data

Physical Properties
  • Melt Mass-Flow Rate, MFR: 20 ± 2 g/10 min at 300℃ / 1.2 kg (GB/T 3682.1-2008)
  • Density: 1200 kg/m³ (GB/T 1033.1-2008)
  • Viscosity-Average Molecular Weight, Mv: 18,000 g/mol (GB/T 36214.2-2018)
  •  

Mechanical Properties
  • Tensile Strength at Yield: 60 MPa (GB/T 1040.1-2018)
  • Elongation at Break: 110% (GB/T 1040.1-2018)
  • Flexural Strength: 95 MPa (GB/T 9341-2008)
  • Izod Impact Strength: 50 kJ/m² (GB/T 1043.2-2018)
Optical Performance
  • Light Transmittance: 88% at 1 mm (GB/T 2410-2008)
  • b Value: ≤1.2 at 2 mm (GB/T 39822-2021)
  • Yellow Index, YI: ≤2.4 at 2 mm (GB/T 39822-2021)
Thermal Properties
  • Heat Deflection Temperature: 123℃ at 1.8 MPa (GB/T 1634.2-2019)
  • Molding Shrinkage: 0.6–0.8% (GB/T 39818-2021)
  • Vicat Softening Temperature: 144℃ (GB/T 1633-2000)
  • Glass Transition Temperature: 147℃ (GB/T 19466.2-2004)
Flammability Rating
  • Limited Oxygen Index, LOI: 27% (GB/T 2406.1-2008)
  • Flame Retardant Grade: V-2 (GB/T 2408-2021)
Processing Parameters
  • Recommended Processing Method: Extrusion molding, injection molding
  • Flow Characteristic: Low viscosity
  • Melt Mass-Flow Rate, MFR: 20 ± 2 g/10 min at 300℃ / 1.2 kg (GB/T 3682.1-2008)
  • Molding Shrinkage: 0.6–0.8% (GB/T 39818-2021)

Use & Applications

  • General use (No additives)
huasheng pc resin

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.