Plastic Granules
YH3400 PA6 High Viscosity Engineering Grade Granules
Yuehua YH3400 is a specific, high-viscosity, engineering-grade Polyamide 6 resin. With uniform, pure white transparent granules. It offers 3.2 relative viscosity, 63 MPa tensile strength, and 220°C melting point, It is widely used for industrial applications, including injection molding, film extrusion, and durable electrical components.
Associated Documents
TDS - Data Sheet
Typical property data
Physical Properties
- Density: 1.15 g/cm³ (GB/T 1103-1986)
- Relative Viscosity: 3.2 (FZ/T 51004-2011)
- Monomer Content: ≤0.5% (FZ/T 51004-2011)
- Moisture Content: ≤0.065% (FZ/T 51004-2011)
Mechanical Properties
- Tensile Strength: 63.0 MPa (GB/T 1040-92)
- Flexural Strength: 73.0 MPa (GB/T 1040-88)
- Flexural Modulus: 1760 MPa (GB/T 1040-88)
- Notched Impact Strength: 7.7 kJ/m² (GB/T 1043-93)
Thermal Properties
- Melting Point: 220°C
- Melt Index: 16.0 (GB/T 3682)
Processing Guide
- Contamination Control: Avoid dust and foreign particles.
- Residence Time: Do not keep molten resin in the barrel for a long time.
- Hot Runner Temperature: Avoid excessive temperature to prevent material degradation.
- Moisture Control: Control moisture before and during high-temperature processing.
Use & Applications
- Industrial filaments
- packaging films
- high-wear-resistant structural parts