Yuehua Baling Chemical YH400

yuehua nylon6 pa6 resin 25kg package

YH400 PA6 Low Viscosity Injection Molding Pellets

Yuehua YH400 is a PA6 Nylon 6 resin from Hunan Yuehua Chemical. It offers good flowability, 2.4 relative viscosity, and 220°C melting point. Ideal for extrusion, injection molding, high glass-fiber PA6 modification, and spinning.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Density: 1.15 g/cm³ (GB/T 1103-1986)
  • Relative Viscosity: 2.4 (FZ/T 51004-2011)
  • Monomer Content: ≤0.5% (FZ/T 51004-2011)
  • Moisture Content: ≤0.065% (FZ/T 51004-2011)
Mechanical Properties
  • Tensile Strength: 70.0 MPa (GB/T 1040-92)
  • Flexural Strength: 95.0 MPa (GB/T 1040-88)
  • Flexural Modulus: 2200 MPa (GB/T 1040-88)
  • Notched Impact Strength: 5.0 kJ/m² (GB/T 1043-93)
Thermal Properties
  • Melting Point: 220°C
  • Melt Index: 58.0 (GB/T 3682)
Processing Guide
  • Flowability: Good
  • Processing Cleanliness: Avoid dust and foreign matter
  • Residence Time: Avoid long melt residence in barrel
  • Hot Runner Temperature: Avoid excessive temperature
  • Moisture Control: Required during high-temperature processing
  • Processing Use: General PA6 molding, glass-fiber reinforcement, spinning

Use & Applications

  • general-purpose PA6 processing
  • high glass-fiber reinforced modification
  • spinning
yuehua nylon6 pa6 resin 25kg package

Send Us a Message