Plastic Granules
YH402SD PA6 Low Viscosity High Wear Resistant Milky White Granules
Yuehua YH402SD is a milky white PA6 nylon resin manufactured primarily by Hunan Yuehua Chemical Industry Co., Ltd. (Baling Chemical Fiber). With uniform granules, good flowability, and a relative viscosity of 2.4, It is designed for high-speed spinning of nylon filament and related PA6 fiber applications.
Associated Documents
TDS - Data Sheet
Typical property data
Physical Properties
- Density: 1.15 g/cm³ (GB/T 1103-1986)
- Relative Viscosity: 2.4 (FZ/T 51004-2011)
- Monomer Content: ≤0.5% (FZ/T 51004-2011)
- Moisture Content: ≤0.065% (FZ/T 51004-2011)
Mechanical Properties
- Tensile Strength: 62 MPa (GB/T 1040-92)
- Flexural Strength: 71 MPa (GB/T 1040-88)
- Flexural Modulus: 1680 MPa (GB/T 1040-88)
- Notched Impact Strength: 5.5 kJ/m² (GB/T 1043-93)
Thermal Properties
- Melting Point: 215°C (Standard not specified)
- Melt Index: 16.0 (GB/T 3682)
Processing Guide
- Clean Handling: Avoid dust and contamination.
- Residence Time: Avoid long melt residence time.
- Temperature Control: Prevent overheating and degradation.
- Moisture Control: Keep moisture controlled during processing.
Use & Applications
- High-speed spinning of nylon filament