Yuehua Baling Chemical YH800

yuehua nylon6 pa6 resin 25kg package

YH800 PA6 Medium Viscosity

Yuehua YH800 is a medium-viscosity PA6 Nylon 6 resin with pure white, transparent, uniform granules. It offers stable processing, low moisture content, and balanced mechanical strength. Suitable for injection molding, flame-retardant modification, fiber spinning, and monofilament production.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Density: 1.15 g/cm³ (GB/T 1103-1986)
  • Relative Viscosity: 2.8 (FZ/T 51004-2011)
  • Monomer Content: ≤0.5% (FZ/T 51004-2011)
  • Moisture Content: ≤0.065% (FZ/T 51004-2011)
Mechanical Properties
  • Tensile Strength: 67.0 MPa (GB/T 1040-1992)
  • Flexural Strength: 89.0 MPa (GB/T 1040-1988)
  • Flexural Modulus: 1990 MPa (GB/T 1040-1988)
  • Notched Impact Strength: 6.0 kJ/m² (GB/T 1043-1993)
Thermal Properties
  • Melting Point: 220°C
  • Melt Index: 38.0 (GB/T 3682)
Processing Guide
  • Clean Handling: Keep Yuehua YH800 away from dust and impurities.
  • Short Residence Time: Avoid long melt residence in the barrel.
  • Hot Runner Control: Avoid excessive hot runner temperature.
  • Moisture Control: Control moisture before high-temperature processing.
  • Processing Use: Injection molding, flame-retardant modification, fiber spinning, and monofilament.

Use & Applications

  • General injection molding
  • Flame-retardant modification
  • Staple fiber spinning
  • Monofilament production