Hyosung Topilene® J801R

hyosung topilene polypropylene 25kg package

Topilene® J801R Homopolymer PP for Small Home Electronics

Hyosung Topilene® J801R is a high-stiffness polypropylene homo polymer engineered for small home electronics. It delivers 140℃ HDT and 155℃ Vicat softening for long-term heat resistance. Flexural modulus reaches 22,500 kg/cm². UL 94HB and UL 746B certified. FDA 21 CFR and EU 10/2011 food-contact compliant.

Associated Documents

TDS - Data Sheet
MSDS - Safety Data Sheet

Typical property data

Physical Properties
  • Density: 0.90 g/cm³ (ASTM D792)
  • Melt Index (230 ℃, 2.16 kg): 20 g/10 min (ASTM D1238)
Mechanical Properties
  • Tensile Strength at Yield: 430 kg/cm² (ASTM D638)
  • Flexural Modulus: 22,500 kg/cm² (ASTM D790)
  • Izod Impact Strength, Notched @ 23 ℃: 3.0 kg·cm/cm (ASTM D256)
  • Rockwell Hardness: 110 R-Scale (ASTM D785)
Thermal Properties
  • Heat Deflection Temperature (0.45 MPa): 140 ℃ (ASTM D648)
  • Vicat Softening Temperature (10 N): 155 ℃ (ASTM D1525)
Flame Characteristics
  • Flammability Rating: UL 94HB compliant
  • Long-Term Thermal Endurance: UL 746B compliant
Injection Molding Processing
  • Feed Zone Temperature: 170 ~ 190 ℃
  • Melting Zone Temperature: 180 ~ 230 ℃
  • Metering Zone Temperature: 200 ~ 250 ℃
  • Die / Nozzle Temperature: 200 ~ 250 ℃
  • Mold Temperature: 30 ~ 50 ℃
  • Injection Pressure: 600 ~ 1,300 Bar
  • Pre-Drying (if condensation present): 80 ~ 100 ℃ for 2 ~ 4 hours, air-circulated
  • Storage Condition: Dry environment below 40 ℃, protected from UV light

Use & Applications

  • Iron housings
  • Toaster housings
  • Coffee maker components
  • Air fryer housings
  • Other small home electronics requiring heat-resistant PP homo polymer