Typical property data
Physical Properties
- Density: 1040 kg/m³ (ISO 1183)
- Water Absorption (Saturated at 23°C): 0.95% (ISO 62)
- Moisture Absorption (Equilibrium at 23°C, 50% RH): 0.24% (ISO 62)
Mechanical Properties
- Tensile Modulus: 2300 MPa (ISO 527)
- Tensile Stress at Yield, 23°C: 44 MPa (ISO 527)
- Tensile Strain at Yield, 23°C: 2.4% (ISO 527)
- Nominal Strain at Break, 23°C: 12% (ISO 527)
- Flexural Strength: 65 MPa (ISO 178)
- Hardness (Ball Indentation): 99 MPa (ISO 2039-1)
- Izod Notched Impact Strength:
- 23°C: 22 kJ/m² (ISO 180/A)
- -30°C: 7 kJ/m² (ISO 180/A)
- Charpy Notched Impact Strength:
- 23°C: 19 kJ/m² (ISO 179/1eA)
- -30°C: 7 kJ/m² (ISO 179/1eA)
- Charpy Unnotched Impact Strength:
- 23°C: 125 kJ/m² (ISO 179/1eU)
- -30°C: 90 kJ/m² (ISO 179/1eU)
Viscosity Properties
Thermal Properties
- Vicat Softening Temperature (ISO 306):
- VST/B/50 (50N, 50°C/h): 95°C
- VST/A/50 (10N, 50°C/h): 102°C
- Heat Deflection Temperature (Annealed at 4 h/80°C) (ISO 75):
- A (1.8 MPa): 92°C
- B (0.45 MPa): 95°C
- Coefficient of Linear Thermal Expansion: 80-110 x10^-6/°C (ISO 11359)
- Thermal Conductivity: 0.17 W/(m·K) (ISO 22007-4)
Electrical Properties
- Volume Resistivity: >10¹³ Ohm·m (IEC 62631-3-1)
- Surface Resistivity: >10¹³ Ohm (IEC 62631-3-1)
Injection Molding Guidelines
- Melt Temperature Range: 220-260°C (ISO 294)
- Mold Temperature Range: 30-80°C (ISO 294)
- Injection Velocity: 200 mm/s (ISO 294)
- Linear Mold Shrinkage: 0.4-0.7% (ISO 294-4)
- Drying Temperature: 80°C
- Drying Time: 2-4 hours
Use & Applications
1. Automotive Interiors
2. Electronics Housings
3. Consumer Appliance Components
4. Toys and Recreational Equipment
5. Electroplating Applications
Features & Benefits
1. Exceptional Flowability for Precision Molding
Simplify the production of complex, thin-wall components. Its high-flow properties (MVR: 34 cm³/10 min at 220°C) ensure superior filling capabilities for intricate designs.
2. Reliable Impact Resistance
Terluran® GP-35 exhibits outstanding room-temperature impact strength (22 kJ/m² at 23°C) while retaining sufficient performance in cold conditions.
3. Heat-Resistant
With a high Vicat softening temperature (102°C), Terluran® GP-35 guarantees excellent thermal distortion resistance.