Plastic Granules
Terluran® HI-10 General Purpose Injection Molding Grade
Terluran® HI-10 is an medium flow, injection molding grade with very high resistance to impact with excellent heat distortion and suitable for injection molding and extrusion.
Typical property data
Physical Properties
- Density: 1030 kg/m³ (ISO 1183)
- Water Absorption:
- Saturated at 23 °C: 1.03% (ISO 62)
- Equilibrium (23 °C / 50% RH): 0.21% (ISO 62)
- Linear Mold Shrinkage: 0.4-0.7% (ISO 294-4)
Mechanical Properties
- Izod Notched Impact Strength:
- 23 °C: 36 kJ/m² (ISO 180/A)
- -30 °C: 14 kJ/m² (ISO 180/A)
- Charpy Impact Strength:
- Notched (23 °C): 35 kJ/m² (ISO 179/1eA)
- Notched (-30 °C): 13 kJ/m² (ISO 179/1eA)
- Unnotched (-30 °C): 140 kJ/m² (ISO 179/1eU)
- Tensile Stress at Yield: 38 MPa (ISO 527)
- Tensile Modulus: 1900 MPa (ISO 527)
- Nominal Strain at Break: 9% (ISO 527)
- Flexural Strength: 56 MPa (ISO 178)
- Hardness, Ball Indentation: 74 MPa (ISO 2039-1)
Viscosity Properties
- Melt Volume Rate: 5.5 cm³/10 min (220 °C / 10 kg) (ISO 1133)
Thermal Properties
- Vicat Softening Temperature:
- VST/A/50 (10N): 103 °C (ISO 306)
- VST/B/50 (50N): 90 °C (ISO 306)
- Heat Deflection Temperature:
- Under Load (1.8 MPa, annealed): 93 °C (ISO 75)
- Under Load (0.45 MPa, annealed): 97 °C (ISO 75)
- Coefficient of Linear Thermal Expansion: 80-110 × 10⁻⁶/°C (ISO 11359)
- Thermal Conductivity: 0.17 W/(m·K) (ISO 22007-4)
Electrical Properties
- Volume Resistivity: >10¹³ Ohm·m (IEC 62631-3-1)
- Surface Resistivity: >10¹³ Ohm (IEC 62631-3-1)
- Relative Permittivity:
- 100 Hz: 2.9 (IEC 62631-2-1)
- 1 MHz: 2.8 (IEC 62631-2-1)
- Dissipation Factor:
- 100 Hz: 54 × 10⁻⁴ (IEC 62631-2-1)
- 1 MHz: 82 × 10⁻⁴ (IEC 62631-2-1)
Injection Molding Guidelines
- Melt Temperature Range: 220-260 °C (ISO 294)
- Mold Temperature Range: 30-80 °C (ISO 294)
- Injection Velocity: Up to 200 mm/s (ISO 294)
- Drying Temperature: 80 °C
- Drying Time: 2-4 hours
Use & Applications
1. Automotive Industry
2. Electronics Industry
3. Consumer Appliances
4. Industrial & Garden Equipment
5. Custom Manufacturing & Injection Molding
Features & Benefits
1. Exceptional Impact Resistance
Designed for high-stress environments, Terluran® HI-10 offers excellent impact strength, even at sub-zero temperatures.
2. Heat Distortion Stability
Engineered for thermal resilience, it delivers reliable performance in high-temperature applications up to 103 °C.