Invista™ U3200 Nylon66

invista pa66 nylon polymer 25kg package

Invista™ U3200 High Viscosity PA66 Resin

INVISTA™ U3200 is a high-performance natural PA66 resin engineered for low viscosity and high flow characteristics. Designed for compounding, it ensures superior wetting-out for glass fibers and solid additives, making it ideal for demanding industrial applications.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Density: 1.14 g/cm³ (ISO 1183)
  • Mold Shrinkage (2.0 mm, parallel): 1.4% (ISO 294-4)
  • Mold Shrinkage (2.0 mm, transverse): 1.4% (ISO 294-4)
  • Water Absorption (24 hours, immersion): Not listed (ISO 62)
  • Moisture Absorption (equilibrium @ 50% RH): 2.5% (ISO 62)
Mechanical Properties
  • Tensile Strength at Yield: 80 MPa (ISO 527)
  • Elongation at Yield: 4.3% (ISO 527)
  • Elongation at Break: 25% (ISO 527)
  • Tensile Modulus: 2950 MPa (ISO 527)
  • Flexural Modulus: 2750 MPa (ISO 178)
  • Flexural Strength (at 3.5% strain): 92 MPa (ISO 178)
  • Notched Charpy (23°C): 6.0 kJ/m² (ISO 179)
  • Notched Charpy (-30°C): 4.0 kJ/m² (ISO 179)
  • Unnotched Charpy (23°C): NB (No Break) kJ/m² (ISO 179)
  • Unnotched Charpy (-30°C): 100 kJ/m² (ISO 179)
  • Notched Izod (23°C): 5.2 kJ/m² (ISO 180)
Viscosity Properties
  • RV in Formic Acid (Nominal): 32 (ASTM D789)
  • VN at 0.5% in Sulfuric Acid (Nominal): 118 mL/g (ISO 307)
  • RV at 1% in Sulfuric Acid (Nominal): 2.3 (Modified ISO 307)
Thermal Properties
  • Melting Temperature (10°C/min): 261°C (ISO 11357)
  • HDT at 0.45 MPa: 198°C (ISO 75)
  • HDT at 1.80 MPa: 69°C (ISO 75)
Injection Molding
  • Drying Temperature: 80°C
  • Drying Time: 4–8 hours
  • Barrel Temperatures:
    • Rear: 255–275°C
    • Middle: 275–295°C
    • Front: 280–295°C
    • Nozzle: 280–295°C
  • Processing Temperature (Melt): 285–295°C
  • Mold Temperature: 50–90°C
  • Back Pressure: 5–30 bar
  • Vent Depth: 0.007–0.04 mm
  • Cushion (Range): 4–6 mm
  • Screw Speed: 50–150 rpm
  • Suggested Moisture Content (Max): 0.20 wt%
  • Suggested Moisture Content (Min): 0.12 wt%

Use & Applications

  • Compounding for Custom Applications
  • Automotive Components
  • Electrical and Electronics (E&E)
  • Industrial Applications
  • Consumer Goods
invista pa66 nylon polymer 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.