Sabic LEXAN™ PC Resin 123M

sabic pc resin 25kg package

SABIC PC Lexan 123M General Purpose Grade

LEXAN 123M is a versatile 18 MFR polycarbonate resin. It features UV stabilization, improved internal mold release for faster cycles, and a UL94 HB flammability rating for reliable performance.

Associated Documents

TDS Americas

Typical property data

Physical Properties
  • Specific Gravity: 1.2 (ASTM D792)
  • Density: 1.19 g/cm³ (ASTM D792)
  • Water Absorption (% at 23°C):
    • 24 hrs: 0.15% (ASTM D570)
    • Saturated: 0.35% (ASTM D570)
    • Equilibrium (100°C): 0.58% (ASTM D570)
  • Melt Flow Rate (300°C/1.2 kgf): 17.5 g/10 min (ASTM D1238)
  • Mold Shrinkage (flow, 3.2 mm): 0.5–0.8% (SABIC method)
Mechanical Properties
  • Tensile Stress (Yield): 63 MPa (ASTM D638)
  • Tensile Stress (Break): 66 MPa (ASTM D638)
  • Tensile Strain (Yield): 7% (ASTM D638)
  • Tensile Strain (Break): 120% (ASTM D638)
  • Flexural Stress: 100 MPa (ASTM D790)
  • Flexural Modulus: 2350 MPa (ASTM D790)
Impact Properties
  • Izod Impact Strength:
    • Unnotched (23°C): 2140 J/m (ASTM D4812)
    • Notched (23°C): 820 J/m (ASTM D256)
    • Notched (-30°C): 200 J/m (ASTM D256)
  • Falling Dart Impact (23°C): 169 J (ASTM D3029)
  • Instrumented Dart Impact Energy (23°C): 77 J (ASTM D3763)
Thermal Properties
  • Vicat Softening Temperature (Rate B/50): 143°C (ASTM D1525)
  • HDT (Heat Deflection Temperature):
    • 0.45 MPa: 137°C (ASTM D648)
    • 1.82 MPa: 132°C (ASTM D648)
  • CTE (Coefficient of Thermal Expansion):
    • Flow Direction: 6.36E-05, 1/°C (ASTM E831)
    • Cross-flow: 6.5E-05, 1/°C (ASTM E831)
  • Thermal Conductivity: 0.19 W/m-°C (ASTM C177)
  • Specific Heat: 1.26 J/g-°C (ASTM C351)
Optical Properties
  • Light Transmission (2.54 mm): 88% (ASTM D1003)
  • Haze (2.54 mm): 1% (ASTM D1003)
  • Refractive Index: 1.586 (ASTM D542)
Flame Characteristics
  • UL94 Rating: HB rated
Injection Molding
  • Drying Parameters:
    • Temperature: 120°C
    • Time: 3–4 hrs (cumulative 48 hrs)
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 280–305°C
  • Nozzle Temperature: 275–300°C
  • Mold Temperature: 70–95°C
  • Back Pressure: 0.3–0.7 MPa
  • Screw Speed: 40–70 rpm
  • Vent Depth: 0.025–0.076 mm

Features & Benefits

Fast, Efficient Moldability

With an 18 MFR, SABIC LEXAN 123M enables faster cycle times and easier flow into intricate molds—ideal for high-volume production with tight tolerances.

Built-In UV Stability

LEXAN™ 123M resin resists yellowing and degradation from sunlight, making it ideal for outdoor or light-exposed parts like electrical housings or automotive trim.

Improved Internal Mold Release

Its self-releasing formulation reduces the need for external mold-release agents, minimizing part defects and reducing downtime in manufacturing.

sabic pc resin 25kg package

Use & Applications

  • Electrical enclosures and components
  • Automotive interior and exterior trim
  • Consumer electronics housings
  • Lighting fixtures and covers
  • Industrial machine guards
  • Transparent or tinted safety panels
  • Small appliance parts
  • Business equipment casings
sabic pc resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.