Sabic LEXAN™ AVP KLL10FR PC Resin

sabic pc resin 25kg package

SABIC AVP KLL10FR Flame Retardant Grade Standard Black

LEXAN™ AVP KLL10FR is a reliable, 10% glass fiber reinforced polycarbonate. It achieves the stringent UL94 V0 and 5VA flame ratings and comes in a standard black color, making it a trusted choice for demanding applications where fire resistance and structural integrity are non-negotiable.

Associated Documents

TDS Americas

Typical property data

Physical Properties
  • Glass Fiber Content: 10% (by description)
Flame Characteristics
  • UL Flame Class Rating: 94V-0 at 1.5 mm (UL 94 by SABIC-IP)

Features & Benefits

Superior Flame Retardancy

This LEXAN AVP KLL10FR resin meets UL94 V0 & 5VA standards, ensuring enhanced safety and compliance for components in electrical and enclosures, reducing fire risk.

Reinforced Structural Integrity

With 10% glass fiber filling, the material offers improved stiffness, dimensional stability, and strength over standard PC, ideal for load-bearing and durable parts.

Consistent Black Color & Processability

Available in a standard black color, it provides uniform appearance and reliable molding performance, streamlining production for aesthetic and functional components.