Plastic Granules
SABIC Lexan AVP ZLL12CP Flame Retardant Grade
LEXAN™ Resin AVP ZLL12CP resin is a wide specification polycarbonate. 12 MFR targeted. UL94 V2 rated. Available in limited opaque colors. Designed for consistent processing and reliable performance.
Associated Documents
TDS Americas
Typical property data
Physical Properties
- Melt Flow Rate: 12 g/10 min (ASTM D1238)
Flame Characteristics
- UL94 Rating: V-2 rated
Injection Molding
- Processing Temperature: 300°C (Implied by melt flow test conditions)
Features & Benefits
Excellent Processability
The balanced 12 MFR ensures smooth flow during injection molding, allowing for easier filling of complex molds, reduced cycle times, and higher production efficiency.
Built-in Flame Retardancy
With its UL94 V-2 rating, this grade provides a recognized level of flame resistance, helping your components meet critical safety requirements without the need for additional additives.
Consistent & Opaque
As a wide-specification resin, it delivers reliable batch-to-batch consistency. Available in standard opaque colors, it is suitable for applications where aesthetics and light shielding are important.