Sabic LEXAN™ PC Resin HF1130

sabic pc resin 25kg package

SABIC Lexan HF1130 UV-stabilized

LEXAN™ HF1130 is a 25 MFR UV-stabilized polycarbonate resin, ideal for delivering robust mechanical performance, excellent impact resistance, and exceptional thermal stability. Designed to meet diverse industry needs, this material ensures reliable performance in demanding applications across multiple sectors.

Associated Documents

TDS Asia
TDS Americas

Typical property data

Physical Properties
  • Specific Gravity: 1.2 (ASTM D792)
  • Mold Shrinkage, Flow (3.2 mm): 0.5–0.7% (SABIC method)
  • Melt Flow Rate (300°C/1.2 kgf): 25 g/10 min (ASTM D1238)
Mechanical Properties
  • Tensile Stress (Yield, Type I, 50 mm/min): 62 MPa (ASTM D638)
  • Tensile Stress (Break, Type I, 50 mm/min): 65 MPa (ASTM D638)
  • Tensile Strain (Break, Type I, 50 mm/min): 110% (ASTM D638)
  • Flexural Stress (Yield, 1.3 mm/min, 50 mm span): 93 MPa (ASTM D790)
  • Flexural Modulus (1.3 mm/min, 50 mm span): 2300 MPa (ASTM D790)
Impact Properties
  • Izod Impact (Notched, 23°C): 640 J/m (ASTM D256)
  • Tensile Impact Strength (Type S): 378 kJ/m² (ASTM D1822)
  • Instrumented Dart Impact Energy (@ Peak, 23°C): 54 J (ASTM D3763)
Thermal Properties
  • HDT (1.82 MPa, 6.4 mm, Unannealed): 126°C (ASTM D648)
  • Relative Temperature Index – Electrical: 100°C (UL 746B)
  • Relative Temperature Index – Mechanical with Impact: 100°C (UL 746B)
  • Relative Temperature Index – Mechanical without Impact: 100°C (UL 746B)
Optical Properties
  • Light Transmission (2.54 mm): 88% (ASTM D1003)
  • Haze (2.54 mm): 1% (ASTM D1003)
Flame Characteristics
  • UL Recognized, Flame Class Rating 94V-2 (1.47 mm): Yes (UL94)
  • UL Yellow Card Link: E207780
Injection Molding
  • Drying Temperature: 120°C
  • Drying Time: 3–4 hrs
  • Drying Time (Cumulative): 48 hrs
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 270–295°C
  • Nozzle Temperature: 265–290°C
  • Front – Zone 3 Temperature: 270–295°C
  • Middle – Zone 2 Temperature: 260–280°C
  • Rear – Zone 1 Temperature: 250–270°C
  • Mold Temperature: 70–95°C
  • Back Pressure: 0.3–0.7 MPa
  • Screw Speed: 40–70 rpm
  • Shot to Cylinder Size: 40–60%
  • Vent Depth: 0.025–0.076 mm

Features & Benefits

High Flow for Complex Molds

LEXAN HF1130 offers a 25 MFR, allowing for faster cycle times and easy molding of intricate, thin-walled parts.

UV Stability for Outdoor Use

UV-stabilized formulation resists discoloration and degradation, making it ideal for exterior housings and outdoor equipment.

Flame-Rated for Electrical Safety

UL94 V2 rating ensures compliance with safety standards, making it suitable for electrical enclosures and internal components.

sabic pc resin 25kg package

Use & Applications

  • Electronics & Appliances
  • Automotive Components
  • Construction & Industrial Equipment
sabic pc resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.