Sabic LEXAN™ PC Resin OQ2720

sabic pc resin

SABIC Lexan OQ2720 UV-stabilized

LEXAN™ OQ2720 resin is a 7.5 MFR polycarbonate. UV stabilized. Produced in dedicated equipment with stringent production control conditions. For ophthalmic or safety lens market. Available in transparent and translucent colors.

Associated Documents

TDS Asia
TDS Americas

Typical property data

Physical Properties
  • Specific Gravity: 1.2 (ASTM D792)
  • Mold Shrinkage (flow, 3.2 mm): 0.5 – 0.7% (SABIC method)
  • Melt Flow Rate (300°C/1.2 kgf): 7.5 g/10 min (ASTM D1238)
Mechanical Properties
  • Tensile Stress, yield (Type I, 50 mm/min): 62 MPa (ASTM D638)
  • Tensile Stress, break (Type I, 50 mm/min): 68 MPa (ASTM D638)
  • Tensile Strain, break (Type I, 50 mm/min): 135% (ASTM D638)
  • Flexural Stress, yield (1.3 mm/min, 50 mm span): 96 MPa (ASTM D790)
  • Flexural Modulus (1.3 mm/min, 50 mm span): 2340 MPa (ASTM D790)
Impact Properties
  • Izod Impact, notched (23°C): 907 J/m (ASTM D256)
  • Tensile Impact Strength (Type S): 640 kJ/m² (ASTM D1822)
  • Instrumented Dart Impact Energy @ peak (23°C): 65 J (ASTM D3763)
Thermal Properties
  • HDT (1.82 MPa, 6.4 mm, unannealed): 132°C (ASTM D648)
Optical Properties
  • Light Transmission (2.54 mm): 89% (ASTM D1003)
  • Haze (2.54 mm): 0.6% (ASTM D1003)
  • Refractive Index: 1.586 (ASTM D542)
  • Yellowness Index: 0 (ASTM D1925)
Injection Molding
  • Drying Temperature: 120°C
  • Drying Time: 3 – 4 hours
  • Drying Time (Cumulative): 48 hours
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 310 – 330°C
  • Nozzle Temperature: 305 – 325°C
  • Zone Temperatures:
    • Front (Zone 3): 310 – 330°C
    • Middle (Zone 2): 300 – 320°C
    • Rear (Zone 1): 290 – 310°C
  • Mold Temperature: 80 – 115°C
  • Back Pressure: 0.3 – 0.7 MPa
  • Screw Speed: 40 – 70 rpm
  • Shot to Cylinder Size: 40 – 60%
  • Vent Depth: 0.025 – 0.076 mm

Features & Benefits

Superior Optical Clarity & Consistency

It delivers high light transmission (89%) with minimal haze, ensuring excellent visual performance for lenses and protective eyewear.

Exceptional Impact Resistance for Safety

Outstanding toughness reduces breakage risk, enhancing product durability in safety-critical applications like industrial lenses.

Enhanced UV Stability & Weatherability

UV-stabilized formulation maintains clarity and prevents yellowing over time, extending product lifespan in both indoor and outdoor use.