Plastic Granules
LG ABS AF362H Flame Retardant Grade
LG ABS AF362H is a flame-retardant ABS resin designed for injection molding. It offers superior V-0 flammability rating at 2.5mm, high thermal resistance, and excellent stability for Blood pressure monitor, oxygen concentrator, pulse monitor.
Typical property data
Physical Properties
- Melt Flow Index: 55 g/10min (220℃, 10kg, ASTM D1238)
Mechanical Properties
- Flexural Strength: 65 MPa (23℃, 10mm/min, 6.4mm, ASTM D790)
- Flexural Modulus: 2400 MPa (23℃, 10mm/min, 6.4mm, ASTM D790)
- Rockwell Hardness: 103 (R-Scale, ASTM D785)
Impact Properties
- Izod Impact Strength (Notched): 22 J/m (6.4mm, 23℃, ASTM D256)
Thermal Properties
- Heat Deflection Temperature: 84℃ (Edgewise, 1.82 MPa, 6.4mm, Unannealed, ASTM D648)
Flame Characteristics
- Flame Retardancy: 2.5mm V-0 rating (UL 94 standard)
Injection Molding (Processing Guidelines)
- Drying Temperature: 80–90℃
- Drying Time: 3–4 hours
- Injection Temperature: 200–230℃
- Mold Temperature: 40–60℃
- Screw Speed: 30–60 rpm
Use & Applications
- Blood Pressure Monitors
- Oxygen Concentrators
- Pulse Monitors
Features & Benefits
Superior Flame Retardant Safety
It achieves a UL94 V-0 rating at 2.5mm thickness, ensuring critical fire safety for sensitive electronic and medical device components, protecting both users and equipment.
Excellent Thermal Resistance
With a Heat Deflection Temperature of 84°C, this ABS resin maintains structural integrity when exposed to heat, ensuring reliable performance in enclosed environments.
High Flow for Easy Processing
A high melt flow index (55 g/10min) allows for easy filling of complex and thin-walled molds, reducing cycle times and improving manufacturing efficiency.