LG Chem ABS AF365HF

lg chem abs resin

LG ABS AF365HF Flame Retardant Grade

LG Chem AF365HF is a high-flow, flame-retardant ABS resin designed for injection molding. It offers excellent thermal stability, a bright white opaque finish, and V-0 fire resistance at 2.0mm, making it ideal for demanding electrical and electronic components.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Melt Flow Index (MFI): 75 g/10min (220°C, 10kg, ASTM D1238)
Mechanical Properties
  • Tensile Strength at Yield: 41 MPa (23°C, 50mm/min, 3.2mm, ASTM D638)
  • Flexural Strength: 63 MPa (23°C, 10mm/min, 6.4mm, ASTM D790)
  • Flexural Modulus: 2400 MPa (23°C, 10mm/min, 6.4mm, ASTM D790)
  • Izod Impact Strength (Notched): 16 J/m (6.4mm, 23°C, ASTM D256)
  • Rockwell Hardness (R-Scale): 105 (ASTM D785)
Impact Properties
  • Izod Impact Strength (Notched): 16 J/m
Thermal Properties
  • Heat Deflection Temperature (HDT): 82°C (Edgewise, 1.82MPa, 6.4mm, Unannealed, ASTM D648)
Flame Characteristics
  • Flame Retardancy: V-0 at 2.0mm thickness
Injection Molding Parameters
  • Drying Temperature: 80–90°C
  • Drying Time: 3–4 hours
  • Injection Temperature: 200–230°C
  • Mold Temperature: 40–60°C
  • Screw Speed: 30–60 rpm

Features & Benefits

Superior Flame Retardant Safety

This LG ABS AF365HF grade achieves a UL94 V-0 rating at just 2.0mm thickness, significantly enhancing product safety and helping your designs meet strict international fire safety regulations for electronics enclosures.

Excellent Thermal Resistance & Stability

With a heat deflection temperature of 82°C, this ABS ABS AF365HF LG Chem material maintains structural integrity in warm environments, preventing deformation in applications like power distribution boxes and internal components.

High Flow for Complex Molding

Its high melt flow rate ensures easy filling of intricate and thin-walled molds, reducing injection pressure and cycle times. This increases production efficiency and minimizes part defects for superior quality.

lg chem abs resin

Use & Applications

  • Electrical Distribution Boxes and Housings
  • Medical Equipment Housings and Components
  • Speaker Grilles and Enclosures
  • Frequency Converters and Power Control Units
lg chem abs resin