LG ABS AF365S Flame Retardant Grade
LG ABS AF365S is a flame retardant ABS resin engineered for extrusion and blow molding. It achieves a superior UL94 V-0 rating at just 2.0mm thickness, making it an ideal, safe, and efficient material choice for demanding applications.
Typical property data
Physical Properties
- Specific Gravity: 1.16 (ASTM D792)
- Mold Shrinkage: 0.4–0.7% at 23℃, 3.2mm (ASTM D955)
- Melt Flow Index: 7.5 g/10min at 220℃, 10 kg (ASTM D1238)
Mechanical Properties
- Tensile Strength at Yield: 47 MPa at 23℃, 50 mm/min, 3.2mm (ASTM D638)
- Tensile Elongation at Yield: Minimum 5% at 23℃, 50 mm/min, 3.2mm (ASTM D638)
- Tensile Elongation at Break: Minimum 15% at 23℃, 50 mm/min, 3.2mm (ASTM D638)
- Flexural Strength: 77 MPa at 23℃, 10 mm/min, 6.4mm (ASTM D790)
- Flexural Modulus: 2550 MPa at 23℃, 10 mm/min, 6.4mm (ASTM D790)
- Rockwell Hardness: R-Scale, 108 (ASTM D785)
Impact Properties
- Izod Impact Strength (Notched):
- 3.2mm: 290 J/m at 23℃ (ASTM D256)
- 6.4mm: 200 J/m at 23℃ (ASTM D256)
Thermal Properties
- Heat Deflection Temperature: 87℃ at 1.82 MPa, 6.4mm, Unannealed (ASTM D648)
Flame Characteristics
- Flammability Ratings (UL 94):
- 1.7mm: V-1
- 2.0mm: V-0, 5VA
- 2.5mm: V-0, 5VA
- 3.0mm: V-0, 5VA
Processing Guide (Extrusion)
- Drying Temperature: 70–80℃
- Drying Time: 3–4 hours
- Moisture Content: ~0.01%
- Extrusion Temperature: 200–230℃
Features & Benefits
Superior Flame Retardant Performance
This material is certified UL94 V-0 at 2.0mm, ensuring critical safety in components where fire resistance is a non-negotiable requirement, protecting both products and end-users.
Excellent Processing Versatility
Optimized for extrusion and blow molding processes, LG Chem AF365S offers excellent melt flow, allowing for easier and more efficient production of large, complex parts like battery housings.
Compliant and Safe Material
This ABS AF365S LG Chem resin is fully compliant with RoHS directives, ensuring your products meet strict international environmental and safety regulations without compromising on performance.
Use & Applications
- Battery Trays for Electric Vehicles and Energy Storage Systems