Typical property data

Physical Properties
  • Specific Gravity: 1.17 (ASTM D792)
  • Mold Shrinkage: 0.4–0.7% (23°C, 3.2 mm, ASTM D955)
  • Melt Flow Index (MFI): 25 g/10 min (220°C, 10 kg, ASTM D1238)
Mechanical Properties
  • Tensile Strength at Yield: 41 MPa (23°C, 50 mm/min, 3.2 mm, ASTM D638)
  • Tensile Elongation at Yield: Minimum 5% (23°C, ASTM D638)
  • Tensile Elongation at Break: Minimum 15% (23°C, ASTM D638)
  • Flexural Strength: 74 MPa (23°C, ASTM D790)
  • Flexural Modulus: 2550 MPa (23°C, ASTM D790)
  • Izod Impact Strength (Notched):
    • 3.2 mm: 200 J/m (23°C, ASTM D256)
    • 6.4 mm: 170 J/m (23°C, ASTM D256)
  • Rockwell Hardness (R-Scale): 108 (ASTM D785)
Impact Properties
  • Izod Impact Strength (Notched):
  • 3.2 mm: 200 J/m (23°C, ASTM D256)
  • 6.4 mm: 170 J/m (23°C, ASTM D256)
Thermal Properties
  • Heat Deflection Temperature (HDT): 87°C (1.82 MPa, Edgewise, 6.4 mm, ASTM D648)
Flame Characteristics
  • Flammability Rating (UL 94):
  • 1.5 mm: V-0
  • 2.0 mm: V-0, 5VA
  • 2.5 mm: V-0, 5VA
  • 3.0 mm: V-0, 5VA
Injection Molding Guidelines
  • Drying Temperature: 70–80°C
  • Drying Time: 3–4 hours
  • Injection Temperature: 200–240°C
  • Mold Temperature: 40–80°C
  • Screw Speed: 30–60 rpm

Features & Benefits

Superior Flame Retardant Performance

This ABS AF366 LG Chem material delivers a critical UL 94 V-0 rating at a thin 1.5mm, ensuring your products meet stringent international safety standards and reduce fire risks.

Excellent Mechanical Strength & Durability

It offers a robust balance of high impact strength and good rigidity, providing structural integrity and damage resistance for protective casings and components in demanding environments.

Easy Processing & High Efficiency

With excellent melt flow characteristics, LG Chem ABS AF366 ensures fast, consistent filling of complex molds, reducing cycle times and improving manufacturing productivity for cost-effective production.

lg chem abs resin

Use & Applications

  • Battery Housings for Power Tools and Consumer Electronics
  • Protective Cases for PCBs and Electrical Components
  • Enclosures for Electrical and Electronic Products
lg chem abs resin

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.