LG Chem ABS AF366A

lg chem abs resin

LG ABS AF366A Flame Retardant Grade

LG ABS AF366A is a flame retardant ABS resin designed for injection molding, offering V-0 flammability rating at 1.5mm and excellent flow properties for high-efficiency production.

Download PDF

Typical property data

Physical Properties
  • Density / Specific Gravity: 1.16 g/cm³ (ASTM D792)
  • Melt Mass-Flow Rate (MFR): 45 g/10 min at 220℃ (ASTM D1238)
  • Molding Shrinkage (Flow): 0.40%−0.70% (23°C, 3.20 mm, injection molded) (ASTM D955)
Mechanical Properties
  • Tensile Strength (Yield): 40.0 MPa (23°C, 3.20 mm, injection molded) (ASTM D638)
  • Tensile Elongation:
    • At Yield: >5.0% (23°C, 3.20 mm, injection molded) (ASTM D638)
    • At Break: >15% (23°C, 3.20 mm, injection molded) (ASTM D638)
  • Rockwell Hardness: 98 R-Scale (ASTM D785)
Impact Properties
  • Notched Izod Impact Strength:
  • 310 J/m (23°C, 3.20 mm, injection molded) (ASTM D256)
  • 200 J/m (23°C, 6.40 mm, injection molded) (ASTM D256)
Thermal Properties
  • Deflection Temperature Under Load (1.8 MPa): 84.0℃ (Unannealed, 6.40 mm, injection molded) (ASTM D648)
  • RTI (Relative Temperature Index):
    • Electrical: 90.0℃ (1.5 – 3.0 mm) (UL 746B)
    • Impact: 90.0℃ (1.5 – 3.0 mm) (UL 746B)
    • Strength: 90.0∘C (1.5 – 3.0 mm) (UL 746B)
Electrical Properties
  • Comparative Tracking Index (CTI): PLC 2 (UL 746A)
  • High Amp Arc Ignition (HAI): PLC 0 (1.5 mm or thicker) (UL 746A)
  • High Voltage Arc Tracking Rate (HVTR): PLC 3 (UL 746A)
  • Hot-wire Ignition (HWI): PLC 2 – PLC 3 (1.5 – 3.0 mm) (UL 746A)
Flame Characteristics
  • Flame Rating:
  • V-0: 1.5 mm and thicker (UL 94, IEC 60695-11-10, -20)
  • 5VA: 2.0 mm and thicker (UL 94, IEC 60695-11-10, -20)
Injection Molding
  • Drying Temperature: 80−90℃
  • Drying Time: 3.0−4.0 hours
  • Processing (Melt) Temperature: 200−230℃
  • Mold Temperature: 40−60℃
  • Screw Speed: 30−60 rpm

Features & Benefits

Superior Flame Retardancy

AF366A achieves UL94 V-0 rating at just 1.5mm, ensuring safety in high-risk electrical and electronic applications without compromising performance.

High Flow for Complex Molds

With a melt flow rate of 45 g/10min, this material fills intricate mold designs quickly, reducing cycle times and improving manufacturing efficiency.

RoHS and Compliance Ready

Fully compliant with EU RoHS directives and free from restricted substances, making it ideal for global markets and environmentally conscious brands.

lg chem abs resin

Use & Applications

  • Electrical and Electronic Housings
  • IT and Office Equipment Enclosures
  • TV and Monitor Bezels and Back Covers
  • Consumer Electronics Components
lg chem abs resin

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.