LG Chem ABS AF367C

lg chem abs resin

LG ABS AF367C Flame Retardant Grade

LG ABS AF367C by LG Chem is a flame retardant ABS resin designed for injection molding, achieving a UL94 V-0 rating at just 2.5mm thickness. Ideal for high-safety electrical and electronic applications.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Density / Specific Gravity: 1.16 g/cm³ (ASTM D792)
  • Melt Mass-Flow Rate (MFR): 45 g/10 min at 220°C/10.0 kg (ASTM D1238)
  • Molding Shrinkage – Flow: 0.40 to 0.70% (23°C, 3.20 mm, Injection Molded, ASTM D955)
Mechanical Properties
  • Tensile Strength (Yield): 39.0 MPa (23°C, 3.20 mm, Injection Molded, ASTM D638)
  • Tensile Elongation (Break): >15% (23°C, 3.20 mm, Injection Molded, ASTM D638)
  • Rockwell Hardness (R-Scale): 100 (23°C, Injection Molded, ASTM D785)
Impact Properties
  • Notched Izod Impact:
  • 310 J/m (23°C, 3.20 mm, Injection Molded, ASTM D256)
  • 200 J/m (23°C, 6.40 mm, Injection Molded, ASTM D256)
Thermal Properties
  • Deflection Temperature Under Load: 84.0°C (1.8 MPa, Unannealed, 6.40 mm, ASTM D648)
  • Relative Temperature Index (RTI):
    • Electrical: 85.0°C (UL 746B, 2.5 mm / 3.0 mm)
    • Impact: 85.0°C (UL 746B, 2.5 mm / 3.0 mm)
    • Strength: 80.0°C (UL 746B, 2.5 mm / 3.0 mm)
Electrical Properties
  • Comparative Tracking Index (CTI): PLC 0 (UL 746A)
  • High Amp Arc Ignition (HAI): PLC 0 (UL 746A)
  • High Voltage Arc Tracking Rate (HVTR): PLC 3 (UL 746A)
  • Hot-wire Ignition (HWI): PLC 3 (UL 746A)
Flame Characteristics
  • Flame Rating: V-0 at 2.5 mm and 3.0 mm (UL 94, IEC 60695-11-10, -20)
Processing Data
  • Drying Temperature: 80 to 90°C
  • Drying Time: 3.0 to 4.0 hours
  • Processing (Melt) Temperature: 200 to 230°C
  • Mold Temperature: 40 to 60°C
  • Screw Speed: 30 to 60 rpm

Features & Benefits

Superior Flame Retardancy

It offers UL94 V-0 rating at 2.5mm, ensuring compliance with strict safety standards for electronics and enclosures.

Excellent Electrical Properties

It features high CTI (PLC 0) and arc resistance, making it suitable for high-voltage components and connectors.

Ease of Processing

High melt flow rate (45 g/10min) allows for fast, efficient injection molding with reduced cycle times.

lg chem abs resin

Use & Applications

  • Electrical and Electronic Housings
  • IT and Office Automation Devices
  • TV and Monitor Enclosures
  • Consumer Electronics Components