LG Chem MABS AT553

lg chem mabs resin 25kg package

LG ABS AT553 Transparent Grade

LG ABS AT553 by LG Chem is a high-performance transparent ABS resin designed for injection molding. It offers excellent permanent antistatic properties (surface resistance 10¹¹Ω) and high clarity, making it ideal for sensitive electronic applications.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Specific Gravity: 1.09 (ASTM D792)
  • Mold Shrinkage: 0.4% ~ 0.7% (ASTM D955)
  • Melt Flow Index: 29 g/10min at 220°C, 10kg (ASTM D1238)
Mechanical Properties
  • Tensile Strength at Yield: 39 MPa at 23°C, 50mm/min, 3.2mm (ASTM D638)
  • Tensile Elongation at Yield: ≥5% at 23°C, 50mm/min, 3.2mm (ASTM D638)
  • Tensile Elongation at Break: ≥15% at 23°C, 50mm/min, 3.2mm (ASTM D638)
  • Flexural Strength: 62 MPa at 23°C, 10mm/min, 6.4mm (ASTM D790)
  • Flexural Modulus: 1800 MPa at 23°C, 10mm/min, 6.4mm (ASTM D790)
  • Izod Impact Strength (Notched):
    • 110 J/m at 23°C, 3.2mm (ASTM D256)
    • 40 J/m at -30°C, 3.2mm (ASTM D256)
    • 110 J/m at 23°C, 6.4mm (ASTM D256)
    • 40 J/m at -30°C, 6.4mm (ASTM D256)
  • Rockwell Hardness: 98 R-Scale (ASTM D785)
Thermal Properties
  • Heat Deflection Temperature:
    • 79°C at Edgewise, 1.82 MPa, 6.4mm, Unannealed (ASTM D648)
    • 87°C at Edgewise, 0.46 MPa, 6.4mm, Unannealed (ASTM D648)
    • 85°C at Edgewise, 1.82 MPa, 6.4mm, Annealed (ASTM D648)
    • 90°C at Edgewise, 0.46 MPa, 6.4mm, Annealed (ASTM D648)
  • Vicat Softening Temperature: 87°C at 50N, 50°C/h (ASTM D1525)
Optical Properties
  • Haze: 4% (ASTM D1003)
  • Luminous Transmittance: 89% at 3.2mm (ASTM D1003)
Electrical Properties

Surface Resistance (Antistatic Property):

Injection Molding
  • Drying Temperature: 70 ~ 80°C
  • Drying Time: 3 ~ 4 hrs
  • Injection Temperature: 200 ~ 250°C
  • Mold Temperature: 40 ~ 80°C
  • Screw Speed: 30 ~ 60 rpm

Features & Benefits

Permanent Antistatic Protection

It drevents dust adsorption and electrostatic discharge, protecting electronic components during production and use.

High Optical Clarity

It delivers 89% luminous transmittance and low haze, enabling visually appealing yet functional transparent enclosures.

Excellent Mechanical Performance

It balances strength, impact resistance, and thermal stability for durable and reliable end-use parts.

lg chem mabs resin 25kg package

Use & Applications

  • Electronic device housings
  • Transparent covers and panels
  • Static-sensitive component carriers
  • Display and touch interface enclosures
  • Industrial and consumer electronics parts
lg chem mabs resin 25kg package

Send Us a Message