LG Chem ABS BM662

lg chem abs resin

LG ABS BM662 Heat Resistant Grade

LG ABS BM662 is a high-performance blow molding ABS resin engineered for demanding automotive exterior parts. It offers an excellent balance of high heat resistance, superior impact strength, and excellent paintability, making it a reliable and cost-effective choice for components like spoilers.

Associated Documents

ISO TDS
ASTM TDS

Typical property data

Physical Properties
  • Specific Gravity: 1.04 (ASTM D792)
  • Mold Shrinkage: 0.4 ~ 0.7% (ASTM D955)
  • Melt Flow Index: 4 g/10 min @ 220℃, 10kg (ASTM D1238)
Mechanical Properties
  • Tensile Strength at Yield: 43 MPa @ 23℃, 50mm/min, 3.2mm (ASTM D638)
  • Tensile Elongation at Break: ≥10% @ 23℃, 50mm/min, 3.2mm (ASTM D638)
  • Flexural Strength: 69 MPa @ 23℃, 15mm/min, 3.2mm (ASTM D790)
  • Flexural Modulus: 2000 MPa @ 23℃, 15mm/min, 3.2mm (ASTM D790)
  • Rockwell Hardness (R-Scale): 101 (ASTM D785)
Impact Properties
  • Izod Impact Strength (Notched):
  • 3.2mm, 23℃: 300 J/m (ASTM D256)
  • 3.2mm, -30℃: 160 J/m (ASTM D256)
  • 6.4mm, 23℃: 300 J/m (ASTM D256)
  • 6.4mm, -30℃: 160 J/m (ASTM D256)
Thermal Properties
  • Heat Deflection Temperature (Unannealed): 95℃ @ 1.82 MPa, 6.4mm (ASTM D648)
  • Vicat Softening Temperature: 104℃, 50N, 50℃/h (ASTM D1525)
Processing Guide
  • Drying Temperature: 80 ~ 90℃
  • Drying Time: 3 ~ 4 hrs
  • Injection Temperature: 230 ~ 270℃
  • Mold Temperature: 40 ~ 80℃
  • Screw Speed: 30 ~ 60 rpm

Features & Benefits

Excellent for Blow Molding

LG ABS BM662 is specifically formulated for blow molding processes, ensuring consistent flow and parison control for creating complex, hollow parts like spoilers with high dimensional stability and uniform wall thickness.

Withstands High Temperatures

This ABS resin maintains its structural integrity in high-heat environments, with a Heat Deflection Temperature of 95°C. This prevents deformation when exposed to summer sun or engine heat, ensuring long-term part performance.

Superior Paintability and Impact Resistance

The surface of BM662 provides excellent adhesion for paints and coatings, allowing for a flawless, durable finish. Combined with high notched impact strength, it helps parts resist chipping, cracking, and abrasion.

lg chem abs resin

Use & Applications

  • Automotive Exterior Spoilers
lg chem abs resin

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.