Typical property data

Physical Properties
  • Specific Gravity: 1.04 (ISO 1183)
  • Mold Shrinkage: 0.4–0.8% at 23°C, 3.2mm (ISO 294-4)
  • Melt Flow Rate: 7 g/10min at 220°C, 10kg (ISO 1133)
Mechanical Properties
  • Tensile Strength at Yield: 47 MPa at 23°C, 50mm/min, 4mm (ISO 527)
  • Tensile Elongation at Yield: Min 5% at 23°C, 50mm/min, 4mm (ISO 527)
  • Tensile Elongation at Break: Min 10% at 23°C, 50mm/min, 4mm (ISO 527)
  • Flexural Strength: 69 MPa at 23°C, 2mm/min, 4mm (ISO 178)
  • Flexural Modulus: 2350 MPa at 23°C, 2mm/min, 4mm (ISO 178)
  • Rockwell Hardness: R107 (ISO 2039)
Impact Properties
  • Izod Impact Strength:
    • Notched, 23°C, 4mm: 23 kJ/m² (ISO 180/1A)
    • Notched, -30°C, 4mm: 10 kJ/m² (ISO 180/1A)
  • Charpy Impact Strength:
    • Notched, 23°C, 4mm: 23 kJ/m² (ISO 179/1eA)
    • Notched, -30°C, 4mm: 10 kJ/m² (ISO 179/1eA)
Thermal Properties
  • Heat Deflection Temperature:
    • At 1.8 MPa, Unannealed: 83°C (ISO 75)
    • At 0.45 MPa, Unannealed: 91°C (ISO 75)
    • At 1.8 MPa, Annealed: 91°C (ISO 75)
    • At 0.45 MPa, Annealed: 96°C (ISO 75)
  • Vicat Softening Temperature: 100°C, 50N, 50°C/h (ISO 306)
Injection Molding Parameters
  • Drying Temperature: 80–90°C
  • Drying Time: 3–4 hrs
  • Injection Temperature: 220–290°C
  • Mold Temperature: 40–80°C
  • Screw Speed: 30–60 rpm

Features & Benefits

Medium Heat Resistance

With a Heat Deflection Temperature of up to 92°C, ER400-C maintains structural integrity in warm environments, making it suitable for applications like appliance housings and automotive interior parts.

Low TVOC & Eco-Friendly

This material meets strict indoor air quality standards with low VOC emissions, ensuring safer use in consumer products and enclosed spaces without compromising performance.

Low Gloss & Aesthetic Flexibility

The matte finish reduces glare and hides fingerprints, ideal for visible surfaces in electronics, furniture, and decorative trim where a premium, non-reflective look is desired.

lg chem abs resin

Use & Applications

  • General Extruded Sheet
  • Edge Band for Furniture and Panels