LG Chem ABS ER400-M

lg chem abs resin

LG ABS ER400-M Heat Resistant Grade

LG ABS ER400-M is a low-gloss, low-VOC ABS resin designed for injection molding. It offers medium heat resistance and is ideal for non-painted interior components, supporting better indoor air quality and streamlined manufacturing.

Associated Documents

ISO TDS
ASTM TDS

Typical property data

Physical Properties
  • Specific Gravity: 1.04 (ISO 1183)
  • Mold Shrinkage: 0.4 ~ 0.8% (23℃, 3.2mm, ISO 294-4)
  • Melt Flow Rate (MFR): 12 g/10min (220℃, 10kg, ISO 1133)
Mechanical Properties
  • Tensile Strength at Yield: 5 MPa (23℃, 50mm/min, 4mm, ISO 527)
  • Tensile Elongation at Break: ≥10% (23℃, 50mm/min, 4mm, ISO 527)
  • Tensile Modulus: 2200 MPa (23℃, 1mm/min, 4mm, ISO 527)
  • Flexural Strength: 62 MPa (23℃, 2mm/min, 4mm, ISO 178)
  • Flexural Modulus: 2000 MPa (23℃, 2mm/min, 4mm, ISO 178)
Impact Properties
  • Izod Notched Impact Strength:
    • 22 kJ/m² (4mm, 23℃, ISO 180/1A)
    • 12 kJ/m² (4mm, -30℃, ISO 180/1A)
  • Charpy Notched Impact Strength:
    • 21 kJ/m² (4mm, 23℃, ISO 179/1eA)
    • 12 kJ/m² (4mm, -30℃, ISO 179/1eA)
Thermal Properties
  • Heat Deflection Temperature (HDT):
    • 82℃ (1.8 MPa, flatwise, 4mm, unannealed, ISO 75)
    • 90℃ (1.8 MPa, flatwise, 4mm, annealed, ISO 75)
    • 90℃ (0.45 MPa, flatwise, 4mm, unannealed, ISO 75)
    • 94℃ (0.45 MPa, flatwise, 4mm, annealed, ISO 75)
  • Vicat Softening Temperature: 100℃ (50N, 50℃/h, ISO 306)
Injection Molding Guidelines
  • Drying Temperature: 80 ~ 90℃
  • Drying Time: 3 ~ 4 hours
  • Injection Temperature: 220 ~ 290℃
  • Mold Temperature: 40 ~ 80℃
  • Screw Speed: 30 ~ 60 rpm

Features & Benefits

Low VOC for Healthier Interiors

ER400-M features very low TVOC emissions, making it an excellent choice for vehicle cockpits and interior trims. This contributes to healthier cabin air quality, meeting stringent environmental standards.

Low Gloss Without Painting

This resin achieves a consistent low-gloss surface directly out of the mold. It eliminates the need for secondary painting, reducing production costs and environmental impact for parts like door trims.

Balanced Strength and Processability

It provides a robust balance of impact strength, heat resistance, and easy flow. This ensures durable performance for interior applications while allowing for efficient, high-quality molding.

lg chem abs resin

Use & Applications

  • Automotive Cockpits & Instrument Panels
  • Interior Door Trims
  • Edge Bands and Profiles
  • Various Interior Components
lg chem abs resin

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.