LG Chem ABS FR500

lg chem abs resin

LG ABS FR500 Flame Retardant Grade

LG ABS FR500 is a premium flame-retardant ABS resin from LG Chem, specifically engineered for injection molding. It achieves a superior UL94 V-0 flammability rating at just 2.0mm thickness, making it an ideal, reliable choice for enhancing safety in sensitive electronic components.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Melt Flow Index: 50 g/10min (220℃, 10kg, ASTM D1238)
Mechanical Properties
  • Tensile Strength at Yield: 43 MPa (23℃, 50mm/min, 3.2mm, ASTM D638)
  • Flexural Strength: 67 MPa (23℃, 10mm/min, 6.4mm, ASTM D790)
  • Flexural Modulus: 2300 MPa (23℃, 10mm/min, 6.4mm, ASTM D790)
  • Rockwell Hardness: 100 R-Scale (ASTM D785)
Impact Properties
  • Izod Impact Strength (Notched): 20 J/m (6.4mm, 23℃, ASTM D256)
Thermal Properties
  • Heat Deflection Temperature: 75℃ (Edgewise, 1.82MPa, 6.4mm, Annealed, ASTM D648)
Flame Characteristics
  • Flammability Rating: V-0 at 2.0mm (UL 94)
Injection Molding
  • Drying Temperature: 75–85℃
  • Drying Time: 2–4 hrs
  • Injection Temperature: 180–240℃
  • Mold Temperature: 40–80℃
  • Screw Speed: 30–60 rpm

Features & Benefits

Superior Flame Retardancy & Safety

This ABS FR500 LG Chem grade delivers a critical UL94 V-0 rating at a thin 2.0mm wall thickness. This enhances end-product safety and helps you meet stringent international fire safety regulations for electronics, reducing potential liability.

Excellent Processing Efficiency

With a high melt flow index (50 g/10min), LG ABS FR500 offers easy flow and fast cycle times in injection molding. This improves production efficiency, reduces energy consumption, and allows for the molding of complex, thin-walled parts with ease.

Compliant & Environmentally Conscious

Certified to comply with EU RoHS Directive, this material is free of restricted substances like lead, cadmium, and phthalates. This ensures your products can access global markets and align with corporate sustainability goals.

lg chem abs resin

Use & Applications

  • Electrical/Electronic Housings and Components
  • Internal Structural Parts for Consumer Electronics
  • Office Machine Components
  • Connectors and Sockets
  • Circuit Board Mounts and Insulators