LG Chem ABS HI135

lg chem abs resin

LG ABS HI135 General Grade

LG ABS HI135 is a high-impact, injection molding grade ABS resin engineered with high rubber content. It delivers exceptional durability and strength, making it the ideal material for demanding protective and consumer applications.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Specific Gravity: 1.04 (ASTM D792)
  • Mold Shrinkage: 0.4–0.7% (ASTM D955)
  • Melt Flow Index: 6 g/10min at 220℃, 10kg (ASTM D1238)
Mechanical Properties
  • Tensile Strength at Yield: 41 MPa (23℃, 50mm/min, 3.2mm, ASTM D638)
  • Tensile Elongation at Break: ≥10% (23℃, 50mm/min, 3.2mm, ASTM D638)
  • Flexural Strength: 65 MPa (23℃, 10mm/min, 6.4mm, ASTM D790)
  • Flexural Modulus: 2100 MPa (23℃, 10mm/min, 6.4mm, ASTM D790)
  • Izod Impact Strength: 460 J/m (Notched, 6.4mm, 23℃, ASTM D256)
  • Rockwell Hardness: 100 (R-Scale) (ASTM D785)
Impact Properties
  • Izod Impact Strength: 460 J/m (Notched, 6.4mm, 23℃, ASTM D256)
Thermal Properties
  • Heat Deflection Temperature: 87℃ (Edgewise, 1.82 MPa, 6.4mm, Unannealed, ASTM D648)
  • Vicat Softening Temperature: 95℃ (50N, 50℃/h, ASTM D1525)
Injection Molding
  • Drying Temperature: 70–80℃
  • Drying Time: 3–4 hours
  • Injection Temperature: 200–250℃
  • Mold Temperature: 40–80℃
  • Screw Speed: 30–60 rpm

Features & Benefits

Exceptional High-Impact Strength

With an Izod impact strength of 460 J/m, LG ABS HI135 LG Chem offers superior toughness, preventing cracks and fractures in products that must withstand sudden impacts and drops.

Excellent Mechanical Rigidity

This material provides a strong flexural modulus of 2100 MPa, ensuring structural integrity and resistance to bending under load for durable and reliable finished parts.

Superior Processing Versatility

ABS HI135 LG Chem features a balanced melt flow (6 g/10min) and wide processing window, enabling easier injection molding, high-quality surface finishes, and increased production efficiency.

lg chem abs resin

Use & Applications

  • Safety Helmets: Its high impact absorption is critical for manufacturing protective headgear that meets safety standards.
  • Miscellaneous Durable Goods: Ideal for a wide range of products requiring toughness, including tool housings, recreational equipment, and consumer appliances.