Typical property data
Physical Properties
- Specific Gravity: 1.04 (ASTM D792)
- Mold Shrinkage: 0.4 ~ 0.7% (ASTM D955)
- Melt Flow Index: 20 g/10 min at 220℃, 10kg (ASTM D1238)
Mechanical Properties
- Tensile Strength at Yield: 42 MPa (ASTM D638, 23℃, 50mm/min, 3.2mm)
- Tensile Elongation at Break: Min 10% (ASTM D638, 23℃, 50mm/min, 3.2mm)
- Flexural Strength: 71 MPa (ASTM D790, 23℃, 10mm/min, 6.4mm)
- Flexural Modulus: 2500 MPa (ASTM D790, 23℃, 10mm/min, 6.4mm)
- Rockwell Hardness: R-Scale 110 (ASTM D785)
Impact Properties
- Izod Impact Strength Notched (3.2mm): 340 J/m (ASTM D256, 23℃)
- Izod Impact Strength Notched (6.4mm): 250 J/m (ASTM D256, 23℃)
Thermal Properties
- Heat Deflection Temperature: 91℃ at 0.46MPa, 6.4mm, unannealed (ASTM D648)
- Vicat Softening Temperature: 101℃ with 50N, 50℃/h (ASTM D1525)
Injection Molding Parameters
- Drying Temperature: 80 ~ 90℃
- Drying Time: 3 ~ 4 hrs
- Injection Temperature: 230 ~ 250℃
- Mold Temperature: 40 ~ 80℃
- Screw Speed: 30 ~ 60 rpm
Features & Benefits
Superior Metal Plating Adhesion
Outstanding chemical bonding with metal coatings ensures chrome and nickel plating stays firmly attached throughout product lifetime, eliminating costly delamination issues.
Enhanced Processing Efficiency
High-flow injection molding properties reduce cycle times and energy consumption while maintaining dimensional stability for complex electroplated parts production.
Exceptional Surface Quality
Smooth, uniform surface finish minimizes pre-plating preparation, reducing processing steps and improving final appearance for premium automotive components.
Use & Applications
- Exterior Trim Components
- Interior Decorative Parts
- Door Handles and Bezels
- Mirror Housings
- Emblems and Badges