LG Chem MABS TR552F

lg chem mabs resin 25kg package

LG ABS TR552F Transparent Grade

LG ABS TR552F is a premium transparent MABS resin engineered for injection molding and extrusion. It delivers an exceptional balance of high optical clarity, superior resistance to whitening, and excellent impact strength for demanding applications.

Associated Documents

ASTM TDS

Typical property data

Physical Properties
  • Specific Gravity: 1.05 (ASTM D792)
  • Mold Shrinkage: 0.4 ~ 0.7% (23℃, 3.2mm) (ASTM D955)
  • Melt Flow Index: 5 g/10min (220℃, 10kg) (ASTM D1238)
Mechanical Properties
  • Tensile Strength at Yield: 40 MPa (23℃, 50mm/min, 3.2mm) (ASTM D638)
  • Tensile Elongation at Yield: 5% (Min) (23℃, 50mm/min, 3.2mm) (ASTM D638)
  • Tensile Elongation at Break: 25% (Min) (23℃, 50mm/min, 3.2mm) (ASTM D638)
  • Flexural Strength: 61 MPa (23℃, 10mm/min, 6.4mm) (ASTM D790)
  • Flexural Modulus: 1700 MPa (23℃, 10mm/min, 6.4mm) (ASTM D790)
  • Rockwell Hardness: 82 (R-Scale) (ASTM D785)
Impact Properties
  • Izod Impact Strength (Notched):
  • 3.2mm at 23℃: 50 J/m (ASTM D256)
  • 3.2mm at -30℃: 20 J/m (ASTM D256)
  • 6.4mm at 23℃: 50 J/m (ASTM D256)
  • 6.4mm at -30℃: 20 J/m (ASTM D256)
Thermal Properties
  • Heat Deflection Temperature (Unannealed):
    • 1.82 MPa, 6.4mm: 79℃ (ASTM D648)
    • 0.46 MPa, 6.4mm: 87℃ (ASTM D648)
  • Heat Deflection Temperature (Annealed):
    • 1.82 MPa, 6.4mm: 85℃ (ASTM D648)
    • 0.46 MPa, 6.4mm: 90℃ (ASTM D648)
  • Vicat Softening Temperature: 87℃ (50N, 50℃/h) (ASTM D1525)
Optical Properties
  • Haze: 1% (ASTM D1003)
  • Luminous Transmittance: 91% (3.2mm) (ASTM D1003)
Processing Guide
  • Drying Temperature: 70 ~ 80℃
  • Drying Time: 3 ~ 4 hours
  • Injection Temperature: 200 ~ 250℃
  • Mold Temperature: 40 ~ 80℃
  • Screw Speed: 30 ~ 60 rpm

Features & Benefits

Exceptional Optical Clarity

It experience crystal-clear transparency with high light transmittance, ideal for products where visual appeal and seeing internal components are critical.

Superior Whitening Resistance

It maintains its pristine clarity and resists stress whitening after bending or impact, ensuring a lasting high-quality finish and product durability.

High Impact Strength & Softness

It offers reliable toughness and a degree of flexibility at various temperatures, providing excellent durability and a premium, soft-touch feel.

lg chem mabs resin 25kg package