Plastic Granules
LG ABS TR557 Transparent Grade
LG ABS TR557 is a premium transparent ABS resin engineered for injection molding. It delivers an exceptional balance of high impact strength and outstanding optical clarity, making it ideal for demanding consumer and industrial applications.
Typical property data
Physical Properties
- Specific Gravity: 1.09 (ASTM D792)
- Mold Shrinkage: 0.4–0.7% (23℃, 3.2mm, ASTM D955)
- Melt Flow Index: 23 g/10min (220℃, 10kg, ASTM D1238)
Mechanical Properties
- Tensile Strength at Yield: 48 MPa (23℃, 50mm/min, 3.2mm, ASTM D638)
- Tensile Elongation at Yield: ≥ 5% (23℃, 50mm/min, 3.2mm, ASTM D638)
- Tensile Elongation at Break: ≥ 15% (23℃, 50mm/min, 3.2mm, ASTM D638)
- Flexural Strength:
- 71 MPa (23℃, 10mm/min, 6.4mm, ASTM D790)
- 77 MPa (23℃, 15mm/min, 3.2mm, ASTM D790)
- Flexural Modulus:
- 2250 MPa (23℃, 10mm/min, 6.4mm, ASTM D790)
- 2300 MPa (23℃, 15mm/min, 3.2mm, ASTM D790)
- Rockwell Hardness: R-Scale 110 (ASTM D785)
Impact Properties
- Izod Impact Strength (Notched):
- 170 J/m (3.2mm, 23℃, ASTM D256)
- 55 J/m (3.2mm, -30℃, ASTM D256)
- 165 J/m (6.4mm, 23℃, ASTM D256)
- 55 J/m (6.4mm, -30℃, ASTM D256)
Thermal Properties
- Heat Deflection Temperature (Unannealed):
- 81℃ (1.82MPa, 6.4mm, ASTM D648)
- 89℃ (0.46MPa, 6.4mm, ASTM D648)
- Heat Deflection Temperature (Annealed):
- 87℃ (1.82MPa, 6.4mm, ASTM D648)
- 92℃ (0.46MPa, 6.4mm, ASTM D648)
- Vicat Softening Temperature: 89℃ (50N, 50℃/h, ASTM D1525)
Optical Properties
- Haze: 1.5% (ASTM D1003)
- Luminous Transmittance: 90% (3.2mm, ASTM D1003)
Processing Guide
- Drying Temperature: 70–80℃
- Drying Time: 3–4 hrs
- Injection Temperature: 200–250℃
- Mold Temperature: 40–80℃
- Screw Speed: 30–60 rpm
Features & Benefits
Exceptional Optical Clarity
TR557 offers high luminous transmittance (90%) and low haze (1.5%), providing crystal-clear visibility for components where aesthetics and display functionality are critical.
Superior Impact Resistance
This material maintains high impact strength (170 J/m at 23°C) even at low temperatures, ensuring product durability and reducing the risk of failure from physical shocks.
Excellent Processing Versatility
With a wide processing window (200-250°C) and good melt flow, TR557 ensures easy molding, high production efficiency, and excellent replication of complex part details.
Use & Applications
- Washing Machine: For transparent lids, detergent dispensers, and control panel covers.
- Refrigerator: For durable and clear vegetable drawers, interior trim, and door handles.
- Electrical/Electronic Products: For protective covers, housings for displays, and transparent structural components.
- Miscellaneous Goods: For a variety of consumer goods requiring a tough, transparent plastic, such as cosmetic cases, office supplies, and home appliances.