Plastic Granules
LG ABS XG569C Transparent Grade
ABS XG569C is a premium transparent ABS resin engineered for injection molding. It delivers an exceptional balance of high optical clarity, superior scratch resistance, and outstanding mechanical strength for demanding electronic applications.
Typical property data
Physical Properties
- Specific Gravity: 1.1 (ASTM D792)
- Mold Shrinkage: 0.4-0.7% at 23°C, 3.2 mm (ASTM D955)
- Melt Flow Index: 11 g/10 min at 220°C, 10 kg (ASTM D1238)
Mechanical Properties
- Tensile Strength at Yield: 59 MPa at 23°C, 50 mm/min, 3.2 mm (ASTM D638)
- Tensile Elongation at Yield: ≥5% at 23°C, 50 mm/min, 3.2 mm (ASTM D638)
- Tensile Elongation at Break: ≥15% at 23°C, 50 mm/min, 3.2 mm (ASTM D638)
- Flexural Strength: 96 MPa at 23°C, 10 mm/min, 6.4 mm (ASTM D790)
- Flexural Modulus: 2850 MPa at 23°C, 10 mm/min, 6.4 mm (ASTM D790)
- Rockwell Hardness: R-Scale 118 (ASTM D785)
Impact Properties
- Izod Impact Strength (Notched):
- 100 J/m at 3.2 mm and 23°C (ASTM D256)
- 30 J/m at 3.2 mm and -30°C (ASTM D256)
- 100 J/m at 6.4 mm and 23°C (ASTM D256)
- 30 J/m at 6.4 mm and -30°C (ASTM D256)
Thermal Properties
- Heat Deflection Temperature (HDT):
- 84°C at 1.82 MPa, 6.4 mm, unannealed (ASTM D648)
- 92°C at 0.46 MPa, 6.4 mm, unannealed (ASTM D648)
- 90°C at 1.82 MPa, 6.4 mm, annealed (ASTM D648)
- 95°C at 0.46 MPa, 6.4 mm, annealed (ASTM D648)
- Vicat Softening Temperature: 92°C at 50N, 50°C/h (ASTM D1525)
Optical Properties
- Haze: 2% (ASTM D1003)
- Luminous Transmittance: 90% at 3.2 mm (ASTM D1003)
Processing Guide
- Drying Temperature: 70-80°C
- Drying Time: 3-4 hours
- Injection Temperature: 200-250°C
- Mold Temperature: 40-80°C
- Screw Speed: 30-60 rpm
Features & Benefits
Superior Optical Clarity & Gloss
XG569C offers over 90% light transmittance, creating crystal-clear components that enhance product aesthetics and user experience without the need for post-processing.
Exceptional Surface Durability
Its high hardness and scratch-resistant properties ensure finished parts maintain a flawless, like-new appearance throughout their lifecycle, reducing wear and tear.
High Strength and Stiffness
This material provides excellent mechanical rigidity and impact resistance, ensuring structural integrity for thin-walled and durable consumer electronics housings.
Use & Applications
- Television Bezels and Framing
- Sound Bar Enclosures
- Remote Control Housings
- Various Electrical/Electronic Product Components