Plastic Granules
LG ABS XG571 Transparent Grade
LG ABS XG571 is a premium transparent ABS resin engineered for injection molding. It delivers an exceptional combination of high translucency, superior surface gloss, and excellent flow characteristics for complex, high-quality components.
Typical property data
Physical Properties
- Specific Gravity: 1.05 (ASTM D792)
- Mold Shrinkage: 0.4–0.7% (ASTM D955)
- Melt Flow Index: 51 g/10min (220℃, 10kg; ASTM D1238)
Mechanical Properties
- Tensile Strength at Yield: 48 MPa (23℃, 50mm/min, 3.2mm; ASTM D638)
- Tensile Elongation at Break: ≥10% (23℃, 50mm/min, 3.2mm; ASTM D638)
- Flexural Strength: 80 MPa (23℃, 10mm/min, 6.4mm; ASTM D790)
- Flexural Modulus: 2650 MPa (23℃, 10mm/min, 6.4mm; ASTM D790)
- Rockwell Hardness (R-Scale): 111 (ASTM D785)
Impact Properties
Impact Properties
- Izod Impact Strength (Notched, 3.2mm): 170 J/m (23℃; ASTM D256)
- Izod Impact Strength (Notched, 6.4mm): 140 J/m (23℃; ASTM D256)
Thermal Properties
- Heat Deflection Temperature: 87℃ (Edgewise, 1.82MPa, 6.4mm, Unannealed; ASTM D648)
- Vicat Softening Temperature: 95℃ (50N, 50℃/h; ASTM D1525)
Processing Guide
- Drying Temperature: 70–80℃
- Drying Time: 3–4 hours
- Injection Temperature: 200–250℃
- Mold Temperature: 40–80℃
- Screw Speed: 30–60 rpm
Features & Benefits
Superior Optical Clarity & Aesthetics
This material offers outstanding translucency and a high-gloss finish, enhancing the visual appeal and perceived value of your products without the need for painting.
Excellent Processing Efficiency
With its high flow rate, LG ABS XG571 fills intricate molds easily, reducing cycle times and improving production efficiency for complex parts with thin walls.
Reliable Mechanical Strength
It provides a robust balance of good impact resistance and structural integrity, ensuring durable and reliable performance in final applications.
Use & Applications
- Air Conditioner Components (e.g., transparent lids, dials)
- Water Purifier Housings (e.g., filter heads, window covers)
- Air Purifier Components
- Electrical/Electronic Product Enclosures