LG Chem ABS XR440

lg chem abs resin

LG ABS XR440 Heat Resistant Grade

LG Chem ABS XR440 is a high-heat ABS resin engineered for interior parts. It offers low gloss and minimal VOC emissions without painting, simplifying your manufacturing process while meeting stringent indoor air quality standards.

Associated Documents

ISO TDS

Typical property data

Physical Properties
  • Specific Gravity: 1.07 (ISO 1183)
  • Mold Shrinkage: 0.4 ~ 0.7% (ISO 294-4)
  • Melt Flow Rate: 6 g/10min at 220℃, 10kg (ISO 1133)
Mechanical Properties
  • Tensile Strength at Yield: 46 MPa (ISO 527, 23℃, 50mm/min, 4mm)
  • Tensile Elongation at Break: Minimum 15% (ISO 527, 23℃, 50mm/min, 4mm)
  • Flexural Strength: 75 MPa (ISO 178, 23℃, 2mm/min, 4mm)
  • Flexural Modulus: 2550 MPa (ISO 178, 23℃, 2mm/min, 4mm)
  • Rockwell Hardness: 114 (R-Scale, ISO 2039)
Impact Properties
  • Izod Impact Strength (Notched, 4mm):
    • 10 kJ/m² at 23℃ (ISO 180/1A)
    • 6 kJ/m² at -30℃ (ISO 180/1A)
  • Charpy Impact Strength (Notched, 4mm):
    • 8 kJ/m² at 23℃ (ISO 179/1eA)
    • 6 kJ/m² at -30℃ (ISO 179/1eA)
Thermal Properties
  • Heat Deflection Temperature (Unannealed):
    • 93℃ at 1.8 MPa (ISO 75)
    • 101℃ at 0.45 MPa (ISO 75)
  • Heat Deflection Temperature (Annealed):
    • 101℃ at 1.8 MPa (ISO 75)
    • 106℃ at 0.45 MPa (ISO 75)
  • Vicat Softening Temperature: 112℃ (ISO 306, 50N, 50℃/h)
Processing Data
  • Drying Temperature: 80 ~ 90℃
  • Drying Time: 3 ~ 4 hrs
  • Injection Temperature: 230 ~ 270℃
  • Mold Temperature: 40 ~ 80℃
  • Screw Speed: 30 ~ 60 rpm

Features & Benefits

Exceptional Heat Resistance

With a Heat Deflection Temperature of 102°C, ABS XR440 LG Chem ensures dimensional stability in high-temperature environments like car interiors under the sun, preventing warping or softening.

Low Gloss, No Painting Needed

The material’s inherent low-gloss surface eliminates the need for costly and environmentally impactful painting processes. This speeds up production and reduces VOC emissions from your factory.

Certified Low VOC Emission

LG ABS XR440 is specifically formulated for low Total Volatile Organic Compound (TVOC) content, helping your final products, such as car cockpits, easily comply with indoor air quality regulations.

lg chem abs resin

Use & Applications

  • Automotive Cockpits & Instrument Panels
  • Door Trim Panels
  • Other Interior Trim Parts