Plastic Granules
LG ABS XR630 Heat Resistant Grade
LG ABS XR630 by LG Chem is a heat-resistant extrusion-grade ABS resin. It offers exceptional resistance to cleaning agents and high temperatures, making it ideal for demanding industrial profiles and components.
Typical property data
Physical Properties
- Specific Gravity: 1.06 (ASTM D792)
- Mold Shrinkage: 0.4 ~ 0.7% (ASTM D955)
- Melt Flow Index: 2.5 g/10min at 220°C, 10kg (ASTM D1238)
Mechanical Properties
- Tensile Strength at Yield: 42 MPa (ASTM D638)
- Tensile Elongation at Break: 15% (Minimum) (ASTM D638)
- Flexural Strength: 68 MPa (ASTM D790)
- Flexural Modulus: 2150 MPa (ASTM D790)
- Rockwell Hardness: R-Scale 104 (ASTM D785)
Impact Properties
- Izod Impact Strength (Notched):
- 310 J/m at 3.2 mm (ASTM D256)
- 250 J/m at 6.4 mm (ASTM D256)
Thermal Properties
- Heat Deflection Temperature:
- 102°C (Edgewise, 1.82 MPa, Unannealed) (ASTM D648)
- 112°C (Edgewise, 0.46 MPa, Unannealed) (ASTM D648)
- Vicat Softening Temperature: 112°C (50N, 50°C/h) (ASTM D1525)
Processing Guide
- Drying Temperature: 80 ~ 90°C
- Drying Time: 3 ~ 4 hrs
- Moisture Content: ~0.01%
- Extrusion Temperature: 180 ~ 250°C
Features & Benefits
Excellent High Heat Resistance
With a Heat Deflection Temperature of up to 102°C, XR630 maintains structural integrity in high-temperature environments, preventing deformation and ensuring long-term product reliability.
Superior Chemical Resistance
This material is specifically designed to withstand harsh cleaning agents, making it perfect for applications requiring frequent cleaning or exposure to chemicals without degrading.
Robust Mechanical Strength
XR630 provides strong tensile and flexural strength, along with good impact resistance, resulting in durable and reliable end-products that can withstand physical stress.
Use & Applications
- Window Profile Insulation Bar