Plastic Granules
Starex® ABF-6220 Antimicrobial Random Copolymer PP
Starex® ABF-6220 is a cutting-edge Random Copolymer PP plastic resin designed for superior functionality, safety, and reliability. Its advanced antimicrobial and anti-fungus properties, combined with excellent weatherability and UV resistance. Ideal for Home Appliances, E&E.
Typical property data
Physical Properties
- Specific Gravity: 1.18 (ISO 1183)
- Melt Flow Index: 23.0 g/10 min (230°C, 2.16 kg; ISO 1133)
- Mold Shrinkage (Flow Direction): 0.3% (ISO 294-4 at 2mm)
- Mold Shrinkage (Transverse Direction): 0.4% (ISO 294-4 at 2mm)
Mechanical Properties
- Tensile Strength (at Break): 50.0 MPa (ISO 527-2, 50 mm/min)
- Tensile Strain (at Break): 5.0% (ISO 527-2, 50 mm/min)
- Tensile Modulus: 2150 MPa (ISO 527-2, 1 mm/min)
- Flexural Strength: 75.0 MPa (ISO 178 at 2 mm/min)
- Flexural Modulus: 2050 MPa (ISO 178 at 2 mm/min)
- Rockwell Hardness: M94 (ISO 2039-2)
Thermal Properties
- Heat Deflection Temperature (at 1.8 MPa): 110°C (ISO 75-2)
- Vicats Softening Temperature (50N, 50°C/h): 115°C (ISO 306)
Processing Parameters
- Processing Technology: Injection Molding
Use & Applications
- Home Appliances
- E&E