Physical Properties
  • Specific Gravity: 1.22 (ISO 1183)
  • Flow Index (230°C, 2.16 kg): 9 g/10 min (ISO 1133)
  • Mold Shrinkage (MD): 0.4% at 2 mm thickness (ISO 294-4)
  • Mold Shrinkage (TD): 0.7% at 2 mm thickness (ISO 294-4)
Mechanical Properties
  • Tensile Strength At Yield: 59 MPa (ISO 527-2)
  • Tensile Strain at Break: 8% (ISO 527-2)
  • Tensile Modulus: 4000 MPa (ISO 527-2)
  • Flexural Strength: 82 MPa (ISO 178)
  • Flexural Modulus: 3700 MPa (ISO 178)
  • Izod Impact Strength Notched: 10 kJ/m² at 23°C (ISO 180 A)
  • Rockwell Hardness: R-Scale: 107 (ISO 2039-2)
Thermal Properties
  • Heat Deflection Temperature (HDT): At 1.8 MPa: 134°C (ISO 75-2)
Flame Characteristics
  • Flammability Rating:
    • UL94, V-0: Thickness 1.5 mm, 3.0 mm
    • UL94, 5VA: Thickness 1.5 mm, 3.0 mm

Use & Applications

  • Electrical housings
  • Switchgear components
  • Consumer appliance parts
  • Flame-rated enclosures for industrial devices
lotte pp 25kg packge

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.