Rastar SKH-126 HIPS

rastar hips resin 25kg package

Rastar SKH-126 HIPS Milky White Pellets Medium-impact

Rastar SKH-126 is a medium-impact, high-flow HIPS resin for fast injection molding. It offers good toughness, milky-white appearance, lower processing temperature, cost efficiency, and reliable use in TV parts, toys, stationery, daily goods, frames, trims, and sheets.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Melt Mass-Flow Rate: 9.5 g/10 min (GB/T 3682)
  • Appearance: Milky white pellets
Mechanical Properties
  • Tensile Strength at Break: 22 MPa (GB/T 1040.2-2006)
  • Elongation at Break: 38% (GB/T 1040)
  • Cantilever Beam Impact Strength: 90 J/m (GB/T 1843)
Thermal Properties
  • Vicat Softening Temperature: 90°C (GB/T 1633)
Processing Parameters
  • MFR / Melt Flow Rate: 4.07 g/10 min (200°C / 5 kg, GB/T 3682.1-2018)
Optical Properties
  • Glossiness: 96% (GB/T 8807)
  • Color / Appearance: Milky white
Processing Parameters
  • Recommended Processing Method: Injection molding
  • Thick-Wall Products / Complex Mold — Feeding Section H-3: 175–188°C
  • Thick-Wall Products / Complex Mold — Plasticizing Section H-2: 185–225°C
  • Thick-Wall Products / Complex Mold — Nozzle H-1: 185–230°C
  • Thin-Wall Products — Feeding Section H-3: 170–180°C
  • Thin-Wall Products — Plasticizing Section H-2: 170–220°C
  • Thin-Wall Products — Nozzle H-1: 180–225°C
Certifications & Compliance
  • Good environmental performance

Use & Applications

  • flat-screen TVs
  • toys
  • stationery
  • daily necessities
  • picture frames
  • decorative strips
  • blister sheets