SABIC® PC Resin PC1000R

sabic pc resin

Sabic PC1000R Injection Molding Grade Heat-stabilized

Sabic PC1000R is a versatile, heat-stabilized polycarbonate with mold release. This medium-low flow grade is engineered for reliability and efficiency in general-purpose injection molding applications.

Associated Documents

TDS Americas
TDS Europe
TDS Asia

Typical property data

Physical Properties (Rheological)
  • Specific Gravity: 1.2 (ASTM D792; ISO 1183)
  • Melt Flow Rate (MFR) at 300°C/1.2 kg: 10 g/10 min (ASTM D1238)
  • Melt Volume Rate (MVR) at 300°C/1.2 kg: 9 cm³/10 min (ISO 1133)
  • Water Absorption (23°C, Saturated): 0.35% (ASTM D570; ISO 62-1)
Mechanical Properties
  • Tensile Stress, Yield: 63 MPa (ASTM D638; ISO 527)
  • Tensile Strain, Yield: 6% (ASTM D638; ISO 527)
  • Tensile Strain, Break: >70% (ASTM D638; ISO 527)
  • Tensile Modulus: 2350 MPa (ASTM D638; ISO 527)
  • Flexural Stress, Yield: 90 MPa (ASTM D790; ISO 178)
  • Flexural Modulus: 2300 MPa (ASTM D790; ISO 178)
  • Hardness (Rockwell, R-Scale): 120 (ASTM D785; ISO 2039-2)
Impact Properties
  • Izod Impact, Notched (23°C): 800 J/m (ASTM D256)
  • Izod Impact, Notched (80×10×3 mm, +23°C): 70 kJ/m² (ISO 180/1A)
  • Izod Impact, Notched (80×10×3 mm, -30°C): 12 kJ/m² (ISO 180/1A)
  • Instrumented Dart Impact Energy (23°C): 65 J (ASTM D3763)
Thermal Properties
  • Vicat Softening Temperature (Rate B/50): 143°C (ASTM D1525; ISO 306)
  • Heat Deflection Temperature (HDT), 0.45 MPa: 138°C (ASTM D648; ISO 75/Bf)
  • Heat Deflection Temperature (HDT), 1.82 MPa: 127°C (ASTM D648; ISO 75/Af)
  • Coefficient of Thermal Expansion (CTE, -40°C to 95°C, flow): 7 × 10⁻⁵ 1/°C (ASTM E831; ISO 11359-2)
  • Thermal Conductivity: 0.2 W/m-°C (ASTM C177; ISO 8302)
Optical Properties
  • Light Transmission (2.54 mm): 88–90% (ASTM D1003)
  • Haze (2.54 mm): <0.8% (ASTM D1003)
  • Refractive Index: 1.586 (ASTM D542; ISO 489)
Electrical Properties
  • Volume Resistivity: >1 × 10¹⁵ Ω·cm (ASTM D257; IEC 60093)
  • Dielectric Strength (1.6 mm): 27 kV/mm (ASTM D149; IEC 60243-1)
  • Relative Permittivity (60 Hz, 1 MHz): 3 (ASTM D150; IEC 60250)
  • Dissipation Factor (60 Hz): 0.001 (ASTM D150; IEC 60250)
  • Dissipation Factor (1 MHz): 0.01 (ASTM D150; IEC 60250)
Flame Characteristics
  • UL 94 Flame Class Rating: 94V-2 (1.6 mm) (UL 94)

Features & Benefits

Superior Impact Resistance & Toughness

With its high notched Izod impact strength, this Sabic PC1000R resin prevents cracking and failure in demanding use, ensuring product durability and longevity for your end-users.

Excellent Thermal Stability & Heat Resistance

Its high Heat Deflection Temperature (HDT) allows parts to maintain structural integrity under elevated temperatures, perfect for applications exposed to heat or requiring sterilization.

Built-in Mold Release for Efficiency

The incorporated mold release agent in SABIC PC Resin PC1000R facilitates easier part ejection, speeding up cycle times and boosting your molding productivity and output.

sabic pc resin

Use & Applications

  • Consumer Electronics Housings
  • Automotive Interior Parts
  • Electrical Connectors and Enclosures