SABIC® PC Resin PC1003R

sabic pc resin

Sabic PC1003R Injection Molding Grade Medium Flow

Sabic PC1003R is a medium-flow, heat and UV-stabilized polycarbonate with built-in mold release. It is a versatile, high-performance plastic designed for reliable general-purpose injection molding, balancing ease of processing with excellent mechanical properties.

Associated Documents

TDS Asia
TDS Europe
TDS Americas
TDS Global

Typical property data

Physical Properties
  • Specific Gravity: 1.2 (ASTM D792, ISO 1183)
  • Water Absorption, Saturated (23°C): 0.35% (ASTM D570, ISO 62-1)
  • Melt Flow Rate (300°C/1.2 kg): 10 g/10 min (ASTM D1238)
  • Mold Shrinkage on Tensile Bar (flow): 0.5–0.7% (SABIC method)
Mechanical Properties
  • Tensile Stress at Yield (50 mm/min): 63 MPa (ASTM D638, ISO 527)
  • Tensile Strain at Yield (50 mm/min): 6% (ASTM D638, ISO 527)
  • Tensile Modulus (1 mm/min): 2350 MPa (ASTM D638, ISO 527)
  • Flexural Stress at Yield (2 mm/min): 90 MPa (ASTM D790, ISO 178)
  • Flexural Modulus (2 mm/min): 2300 MPa (ASTM D790, ISO 178)
  • Hardness (Rockwell R): 120 (ASTM D785, ISO 2039-2)
Impact Properties
  • Izod Impact, Notched (+23°C): 800 J/m (ASTM D256), 70 kJ/m² (ISO 180/1A)
  • Izod Impact, Notched (-30°C): 12 kJ/m² (ISO 180/1A)
  • Instrumented Dart Impact Energy at Peak (+23°C): 65 J (ASTM D3763)
Thermal Properties
  • Vicat Softening Temperature (Rate B/50): 143°C (ASTM D1525, ISO 306)
  • Heat Deflection Temperature (HDT), 0.45 MPa: 138°C (ASTM D648, ISO 75/Bf)
  • Heat Deflection Temperature (HDT), 1.82 MPa: 127°C (ASTM D648, ISO 75/Af)
  • Coefficient of Thermal Expansion (CTE, Flow): 7×10−57 \times 10^{-5} 1/°C (ASTM E831, ISO 11359-2)
  • Thermal Conductivity: 0.2 W/m-°C (ASTM C177, ISO 8302)
Optical Properties
  • Light Transmission (2.54 mm): 88–90% (ASTM D1003)
  • Haze (2.54 mm): <0.8% (ASTM D1003)
  • Refractive Index: 1.586 (ASTM D542, ISO 489)
Electrical Properties
  • Volume Resistivity: >1×10151 \times 10^{15} Ω·cm (ASTM D257, IEC 60093)
  • Dielectric Strength (1.6 mm): 27 kV/mm (ASTM D149, IEC 60243-1)
  • Relative Permittivity (60 Hz): 3 (ASTM D150, IEC 60250)
  • Dissipation Factor (60 Hz): 0.001 (ASTM D150, IEC 60250)
Flame Characteristics
  • UL Flame Class Rating: 94V-2 (1.6 mm) (UL 94)

Features & Benefits

Superior Impact Resistance & Toughness

With its notch-insensitive nature and high ductility, Sabic PC1003R produces incredibly tough parts that resist cracking and withstand sudden impacts, reducing breakage and product failure in demanding environments.

Excellent Thermal & UV Stability

This resin maintains its structural integrity and appearance under high temperatures and prolonged sun exposure, ensuring long-term performance and color stability for both indoor and outdoor applications.

Enhanced Mold Release & Processability

The built-in mold release agent facilitates easier part ejection and shorter cycle times, boosting your production efficiency and reducing the need for external release agents that can contaminate molds.

sabic pc resin

Use & Applications

  • Consumer Electronics Housings
  • Automotive Interior Components
  • Electrical Enclosures and Connectors
  • Household Appliances and Tools
  • Various Durable Consumer Goods
sabic pc resin

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.