SABIC® PC Resin PC1804R

sabic pc resin

Sabic PC1804R Injection Molding Grade Medium-high flow Heat-stabilized

Sabic PC1804R is a medium-high flow, heat-stabilized polycarbonate with mold release. Ideal for general-purpose molding, it offers excellent processability and is food-contact compliant in most regions.

Associated Documents

TDS Asia
TDS Europe
TDS MEA

Typical property data

Physical Properties
  • Specific Gravity: 1.2 (ASTM D792, ISO 1183)
  • Melt Flow Rate (MFR): 18 g/10 min at 300°C/1.2 kg (ASTM D1238)
  • Water Absorption (23°C, Saturated): 0.35% (ASTM D570, ISO 62-1)
  • Mold Shrinkage (Flow): 0.5–0.7% (SABIC Method)
Mechanical Properties
  • Tensile Stress (Yield): 63 MPa (ASTM D638, ISO 527)
  • Tensile Strain (Break): >70% (ASTM D638, ISO 527)
  • Tensile Modulus: 2350 MPa (ASTM D638, ISO 527)
  • Flexural Stress (Yield): 90 MPa (ASTM D790, ISO 178)
  • Flexural Modulus: 2300 MPa (ASTM D790, ISO 178)
  • Rockwell Hardness (R-scale): 120 (ASTM D785, ISO 2039-2)
Impact Properties
  • Izod Impact Strength (Unnotched, 23°C): NB (No Break) (ASTM D4812, ISO 180/1U)
  • Izod Impact Strength (Notched, 23°C): 700 J/m (ASTM D256); 70 kJ/m² (ISO 180/1A)
  • Izod Impact Strength (Notched, -30°C): 12 kJ/m² (ISO 180/1A)
  • Instrumented Dart Impact Energy (Peak, 23°C): 65 J (ASTM D3763)
Thermal Properties
  • Vicat Softening Temperature (B/50): 141°C (ASTM D1525, ISO 306)
  • HDT (0.45 MPa, 3.2 mm): 135°C (ASTM D648, ISO 75/Bf)
  • HDT (1.82 MPa, 3.2 mm): 124°C (ASTM D648, ISO 75/Af)
  • Thermal Conductivity: 0.2 W/m·°C (ASTM C177, ISO 8302)
  • Coefficient of Thermal Expansion (Flow): 7.E-05 1/°C (ASTM E831, ISO 11359-2)
Optical Properties
  • Light Transmission (2.54 mm): 88–90% (ASTM D1003)
  • Haze (2.54 mm): <0.8% (ASTM D1003)
  • Refractive Index: 1.586 (ASTM D542, ISO 489)
Electrical Properties
  • Volume Resistivity: >1.E+15 Ω·cm (ASTM D257, IEC 60093)
  • Dielectric Strength (1.6 mm): 27 kV/mm (ASTM D149, IEC 60243-1)
  • Relative Permittivity: 3 (60 Hz, 1 MHz) (ASTM D150, IEC 60250)
  • Dissipation Factor: 0.001 (60 Hz), 0.01 (1 MHz) (ASTM D150, IEC 60250)
Flame Characteristics
  • UL Flame Rating: 94V-2 (1.5 mm) (UL 94)
Injection Molding
  • Drying Temperature: 120°C
  • Drying Time: 2–4 hours
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 280–300°C
  • Mold Temperature: 80–100°C
  • Nozzle Temperature: 270–290°C

Features & Benefits

Excellent Flow for Complex Molds

Its medium-high flow rate ensures easy filling of intricate molds, reducing cycle times and short shots for higher productivity and lower reject rates.

Superior Impact Strength & Durability

This resin offers outstanding toughness, resisting cracks and breaks from drops or impacts, which is crucial for creating durable and long-lasting consumer and industrial components.

Good Heat Resistance & Stability

With a heat deflection temperature of 124°C at 1.82 MPa, it maintains structural integrity in high-temperature environments, ensuring part reliability during use and assembly.

sabic pc resin

Use & Applications

  • Consumer Electronics Housings
  • Automotive Interior Components
  • Household Appliances Parts
  • Food Contact Containers and Lids
  • Various Industrial and Consumer Goods
sabic pc resin

Send Us a Message