Plastic Granules
XENOY™ Resin 1731HS Impact-modified PC PBT Raw Material Pellets
Associated Documents
TDS - Asia
Typical property data
Physical Properties
Density: 1.2 g/cm³ (ISO 1183)
Moisture Absorption at 23°C / 50% RH: 0.143% (ISO 62)
Water Absorption at 23°C / Saturated: 0.431% (ISO 62-1)
Mold Shrinkage, Flow, 3.2 mm: 0.6 – 0.8% (SABIC Method)
Mold Shrinkage, Cross Flow, 3.2 mm: 0.6 – 0.8% (SABIC Method)
Melt Volume Rate, 250°C / 5.0 kg: 8 cm³/10 min (ISO 1133)
Melt Flow Rate, 250°C / 5.0 kg: 9 g/10 min (ISO 1133)
Moisture Absorption, 23°C / 50% RH / 24 hrs: 0.069% (ASTM D570)
Water Absorption, 23°C / 24 hrs: 0.241% (ASTM D570)
Mechanical Properties
Tensile Stress at Break, 5 mm/min: 51 MPa (ISO 527)
Tensile Strain at Break, 5 mm/min: 100% (ISO 527)
Tensile Modulus, 1 mm/min: 2100 MPa (ISO 527)
Flexural Stress at Break, 2 mm/min: 78 MPa (ISO 178)
Flexural Modulus, 2 mm/min: 2000 MPa (ISO 178)
Impact Properties
Notched Izod Impact, 80 × 10 × 4 mm, +23°C: 60 kJ/m² (ISO 180/1A)
Notched Izod Impact, 80 × 10 × 4 mm, -30°C: 25 kJ/m² (ISO 180/1A)
Notched Izod Impact, 80 × 10 × 4 mm, -40°C: 19 kJ/m² (ISO 180/1A)
Thermal Properties
Vicat Softening Temperature, Rate B/50: 125°C (ISO 306)
Vicat Softening Temperature, Rate B/120: 127°C (ISO 306)
Heat Deflection Temperature, HDT/Af, 1.8 MPa, Flatwise, 80 × 10 × 4 mm, Span 64 mm: 95°C (ISO 75/Af)
Coefficient of Thermal Expansion, -40°C to 40°C, Flow: 8.6E-05 1/°C (ISO 11359-2)
Coefficient of Thermal Expansion, -40°C to 40°C, Cross Flow: 8.5E-05 1/°C (ISO 11359-2)
Injection Molding Processing
Drying Temperature: 110°C
Drying Time: 3 – 5 hrs
Cumulative Drying Time: 8 hrs
Maximum Moisture Content: 0.02%
Melt Temperature: 255 – 270°C
Nozzle Temperature: 250 – 265°C
Front Zone 3 Temperature: 255 – 270°C
Middle Zone 2 Temperature: 250 – 265°C
Rear Zone 1 Temperature: 240 – 260°C
Mold Temperature: 65 – 75°C
Back Pressure: 0.3 – 0.6 MPa
Screw Speed: 50 – 80 rpm
Shot to Cylinder Size: 50 – 80%
Vent Depth: 0.013 – 0.02 mm
Use & Applications
- Automotive Exteriors: Bumper systems, body panels, and mirror housings.
- Outdoor Gear: Housings and protective covers exposed to weather.
- Industrial Parts: Tough mechanical enclosures requiring high dimensional stability.