XENOY™ Resin PC PBT RCX201

sabic xenoy pc pbt

XENOY™ Resin PC PBT RCX201 for Durable Molded Parts

XENOY™ Resin RCX201 is a SABIC PC/PBT resin with balanced strength, toughness, and heat resistance. It offers 52 MPa tensile yield stress, 392 J/m notched Izod impact at 23°C, and 130°C HDT for durable molded parts.

Associated Documents

TDS - Asia

Typical property data

Physical Properties
  • Specific Gravity: 1.23 (ASTM D792)
  • Mold Shrinkage, Flow, 3.2 mm: 0.5–0.8% (SABIC Method)
Mechanical Properties
  • Tensile Stress, Yield: 52 MPa (SABIC – Japan Method)
  • Tensile Strain, Break: 200–200% (SABIC – Japan Method)
  • Flexural Stress: 82 MPa (ASTM D790)
  • Flexural Modulus: 2150 MPa (ASTM D790)
Impact Properties
  • Izod Impact, Notched, 23°C: 392 J/m (ASTM D256)
  • Izod Impact, Notched, -30°C: 50 J/m (ASTM D256)
Thermal Properties
  • HDT, 1.82 MPa, 3.2 mm, Unannealed: 130°C (ASTM D648)
  • CTE, -30°C to 30°C: 6.0E-05 1/°C (TMA)

Use & Applications

  • Automotive parts
  • Electrical housings
  • Industrial equipment components