Plastic Granules
Sinopec 525 GPPS Food Contact Grade Medium Flow
Sinopec 525 is a natural GPPS resin from Sinopec GuangZhou Company. It provides medium flow, melt index of 5.0–11.0 g/10 min, tensile stress at break ≥34 MPa, Charpy impact strength ≥6.5 kJ/m², Vicat softening temperature ≥80 ℃, and light transmittance ≥85%. Sinopec 525 GPPS is suitable for household utensils, injection-molded small containers, medical articles, and laboratory articles.
Associated Documents
TDS - Data Sheet
RoHS
MSDS
FDA report
Typical property data
Physical Properties
- Pellet Appearance / Colored Pellets: ≤40 count/kg (SH/T 1541-2006)
- Melt Mass Flow Rate / Melt Index: 5.0–11.0 g/10 min (GB/T 3682-2000)
- Residual Styrene Monomer Content: ≤800 mg/kg (GB/T 16867-1997)
- Molding Shrinkage: Data supplied by supplier % (GB/T 17037.4-2003)
- Color: Natural / Transparent pellets
Mechanical Properties
- Tensile Stress at Break: ≥34 MPa (GB/T 1040.2-2006)
Thermal Properties
- Vicat Softening Temperature: ≥80 ℃ (GB/T 1633-2000, Method B50)
- Deflection Temperature Under Load: ≥75 ℃ (GB/T 1634.2-2004)
Optical Properties
- Light Transmittance: ≥85% (GB/T 2410-2008)
Processing Parameters
- Flow Behavior: Medium flow
- Processing Performance: Excellent processing properties
- Recommended Processing: Injection molding
Use & Applications
- household utensils
- injection-molded small containers
- medical and laboratory articles