Plastic Granules
Sinopec PPH M17 Medium–high Flow Grade
Sinopec PP M17 is a medium-high flow Homopolymer PP resin for general injection molding. It offers 16–17 g/10 min MFR, 31–33 MPa tensile yield strength, and 1280–1340 MPa flexural modulus. Good flow supports stable molding and efficient production.
Associated Documents
TDS - Data Sheet
Typical property data
Physical Properties
- Melt Flow Rate: 16–17 g/10 min (Test standard not specified in datasheet)
- Isotactic Index: 93%
- Ash Content: 0.015%
- Color Form: Natural / original color material
- Flow Classification: Medium–high flow
Mechanical Properties
- Tensile Yield Strength: 31–33 MPa
- Notched Izod Impact Strength: 20 kJ/m² at 23°C
- Flexural Modulus: 1280–1340 MPa
Thermal Properties
- Heat Deflection Temperature: 87°C
Use & Applications
General-purpose injection molded products